Seismic vulnerability in steel buildings

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic vulnerability in steel buildings

Author(s): Moreno González, R.; Bairán García, J. M.; Rodas Aldana, W.A.

Publication: ACHE

Volume: 62

Issue: 261

Appears on pages(s): 69 - 80

Keywords: vulnerability, capacity, fragility, seismic damage, steel building.

DOI:

Date: 1/5/2011

Abstract:
This work is a contribution to the analysis of the seismic behaviour in steel buildings and considering the seismic risk analysis in an urban area situated in a low seismic hazard region and in a moderate seismic hazard region. The vulnerability and the seismic risk of a steel building are evaluated by means of capacity based spectrum method. The structural model used in the analysis corresponds to a real steel building of 8 storeys with concrete slab. The main objective is obtaining, for this building, the capacity and fragility curves. Two specific seismic scenarios, one for the city of Barcelona and another for Almeria, are considered. Taking into account all these results, the probability damage matrices are obtained. The results show, for this typology, a good behaviour for the acceleration of Barcelona, however, for a bigger acceleration, like Almeria, the damages expected are moderate.