Ductile-brittle transition and minimum reinforcement ratio in lightly reinforced concrete columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Ductile-brittle transition and minimum reinforcement ratio in lightly reinforced concrete columns

Author(s): Porras-Soriano, R.; Ruiz Carmona, J.; Yu, R.C.; Ruiz López, G.

Publication: ACHE

Volume: 64

Issue: 268

Appears on pages(s): 75 - 88

Keywords: reinforced concrete, buckling, reinforcement ratio, ductile-brittle transition, size effect.

DOI:

Date: 1/3/2013

Abstract:
This work reports the results of a series of tests performed on lightly reinforced concrete panels subjected to buckling load. We disclose the sensitivity of the specimens to changes in the slenderness, the load eccentricity and the reinforcement ratio. These tests were performed on scaled reinforced concrete specimens in order to reproduce the behavior of lightly reinforced concrete elements subjected to buckling. During these tests, load applied and displacements at mid-span of the specimen (additional eccentricity) were measured; the element response even after the peak load was captured. The paper proposes a simple classification of the element behavior as function of the slenderness and load eccentricity. Based on this classification, the Spanish code requirements of minimum mechanical reinforcement to avoid brittle failure in compressed elements are reviewed.