Auscultation of three road bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Auscultation of three road bridges

Author(s): Astudillo Pastor, R.; Alcalá Sánchez, J.L.

Publication: ACHE

Volume: 45

Issue: 190

Appears on pages(s): 93 - 102

Keywords:

DOI:

Date: 1/1/1994

Abstract:
Three prestressed conccrete structures were studied for determining the causes of their patology: extensive deck cracking without evidence of tensional origin. Theoretical and experimental analysis were performed. The experimental work consisted in dynamic auscultation, vibrating tendon tests and core samples testing with chemical and mineralogy analysis. Deterioration by several mechanical causes were discarded and finally expansive mineral formations were located and described as origin of damage.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »