A practical and safe formulation of the analysis of punching shear of slabs sufficiently adapted to their actual behaviour

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A practical and safe formulation of the analysis of punching shear of slabs sufficiently adapted to their actual behaviour

Author(s): Regalado Tesoro, F.

Publication: ACHE

Volume: 54

Issue: 227

Appears on pages(s): 113 - 119

Keywords:

DOI:

Date: 1/1/2003

Abstract:
We believe it is posible to set up a simple formulation on punching shear of slabs, considering the critical perimeter at 0,5 d from the edge of the columns and varying the shear strength of the concrete. Such variation is set up depending on where the slab columns are located: internal columns, edge columns and corner columns.