Comparison of Test Methods and Effect of Adhesive Coverage on Sustainability of Reinforced Concrete Structures Strengthened with Externally Bonded CFRP Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Comparison of Test Methods and Effect of Adhesive Coverage on Sustainability of Reinforced Concrete Structures Strengthened with Externally Bonded CFRP Materials

Author(s): Jennifer Eisenhauer Tanner, David Mukai, Jiangang Deng, and Charles W. Dolan

Publication: Symposium Paper

Volume: 322

Issue:

Appears on pages(s): 8.1-8.12

Keywords: CFRP, repair, strength, sustainability, durability, accelerated ageing

DOI: 10.14359/51706959

Date: 6/18/2018

Abstract:
Sustainability of CFRP materials is evaluated based on their long-term capacities that can be decreased by environmental exposure. Researchers regularly accelerate this process by various forms of hygrothermal conditioning. Results of both flexural and tension tests are presented. A comparison of flexural and direct tension test methods is proposed and compared to those obtained by other investigators. In addition, a simple predictive model is introduced. Accelerated ageing tests indicate that the sustainability of carbon fiber reinforced polymer (CFRP) repair systems is impacted by the coverage rate of adhesives. Test results indicate no change in strength for specimens with 91 to 233 percent of the manufacturer’s recommended adhesive application while accelerated ageing tests show a markedly lower strength for specimens with less than the manufacturer’s recommended coverage.

Related References:

AASHTO T97-03, 2003, “Standard Method of Test for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading”, American Association of State Highway and Transportation Officials, Washington.

ACI 440.2R-08, 2008. Guide for the Design and construction of Externally Bonded FRP Systems for Strengthening Concrete Structures, ACI Committee 440, Farmington Hills, MI.

ACI 440.9R-15, 2015. Guide to Accelerated Conditioning Protocols for Durability Assessment of Internal and External FRP Reinforcement, ACI Committee 440, Farmington Hills, MI.

ASTM C78, 2010. Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading, Annual Book of ASTM Standards, ASTM International, West Conshohocken, PA.

ASTM D 4541, 2009, “Standard Test Method for Pull-Off Strength of Coatings Using Portable Adhesion Testers, Annual Book of ASTM Standards, ASTM International, West Conshohocken, PA.

Bank, L.C., Gentry T.R., Thompson B.P, Russell, J.S., 2003, "A model specification for FRP composites for civil engineering structures." Construction and Building Materials 17, No. 6 pp. 405-437.

Chen, Y., Davalos, J. Ray, I., 2006, "Durability prediction for GFRP reinforcing bars using short-term data of accelerated aging tests." Journal of Composites for Construction 10, No. 4, pp. 279-286.

Deng, J., 2008, “Durability of Carbon Fiber Reinforced Polymer (CFRP) Repair/Strengthening of Concrete Beams”, PhD Dissertation, University of Wyoming.

Gartner A.L., Douglas E.P., Dolan C.W., Hamilton, H.R., 2011, “Small Beam Bond Test Method for CFRP Composites Applied to Concrete,” ASCE Journal of Composites in Construction, V. 15, No.1, pp. 52-61.

Grace N. F., and Singh, S. B., 2005, “Durability Evaluation of carbon Fiber-Reinforced Polymer Strengthened Concrete Beams: Experimental Study and Design”. ACI Structural Journal, Vol. 102, No. 1, pp. 40-53.

Horiguchi, T., Saeki, N., 1997, Effect of Test Methods and Quality of Concrete on Bond Strength of CFRP Sheet, Non-Metallic (FRP) Reinforcement for Concrete Structures, Proceedings of the Third International Symposium, Vol.1, pp. 265-270.

Karbhari, V., Abanilla, M., 2007, "Design factors, reliability, and durability prediction of wet layup carbon/epoxy used in external strengthening." Composites Part B: Engineering 38, No. 1, pp. 10-23.

Malvar, L.J., Joshi,N.R., Beran, J.A., Novison, T., 2003, “Environmental Effects on the Short-Term Bond of Carbon Fiber-Reinforced Polymer (CFRP) Composites.” Journal of Composites for Construction, Vol. 7, No. 1, pp. 58-63.

NCHRP Report 155, 2008, Dolan C.W., Tanner J.E., Hamilton H.R., Mukai D.J., Douglas E., “Design Guidelines for the Durability of Bonded CFRP Repair Strengthening of Concrete Beams.” National Cooperative Highway Research Program (NCHRP), Final Report, 63 pp.

Phani, K.K., Bose, N.R., 1986, "Temperature dependence of hydrothermal ageing of CSM-laminate during water immersion." Composites science and technology 29, No. 2, pp. 79-87.

Tatar, Jovan, and H. R. Hamilton, (2015a) "Implementation of Bond Durability in the Design of Flexural Members with Externally Bonded FRP." Journal of Composites for Construction, 04015072.

Tatar, Jovan, and H. R. Hamilton, (2015b) "Bond durability factor for externally bonded CFRP systems in concrete structures." Journal of Composites for Construction 04015027.

Toutanji, H.A., Gomez, W., 1997, Durability Characteristics of Concrete Beams Externally Bonded with FRP Composite Sheets, Cem. Concr. Compos. 19, pp. 351-358.

Tuakta, C., Büyüköztürk, O., 2011, "Conceptual model for prediction of FRP-concrete bond strength under moisture cycles." Journal of Composites for Construction, 15, No. 5, pp. 743-756.