Strengthening of Reinforced Concrete Beams with GFRCM

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Strengthening of Reinforced Concrete Beams with GFRCM

Author(s): Rizwan Azam, Ayman Shihata, Khaled A. Soudki and Jeffrey S. West

Publication: Symposium Paper

Volume: 322

Issue:

Appears on pages(s): 7.1-7.16

Keywords: Reinforced Concrete, FRCM, TRM, TRC, glass, fabric, cementitious, bond, shear, corrosion

DOI: 10.14359/51706958

Date: 6/18/2018

Abstract:
This paper presents the results of an experimental study conducted to investigate the effectiveness of a glass fabric reinforced cementitious matrix (GFRCM) composite system to strengthen reinforced concrete (RC) beams. A total of fifteen beams were tested in two groups: Group A was designed to investigate the use of GFRCM to rehabilitate corrosion damaged tension lap splices in RC beams. Group B was designed to investigate the use of GFRCM to strengthen shear critical RC beams. The test results demonstrated that GFRCM is a promising system to enhance the load carrying capacity of RC beams.