Title: 329.1T-18: TechNote: Minimum Cementitious Materials Content in Specifications

Author(s): ACI Committee 329

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 4

Keywords: 329.1, 3291T

DOI:

Date: 5/1/2018

Abstract:
This TechNote discusses the implications of minimum cementitious materials content in project specifications (NRMCA 2015a). Prescriptive specifications for concrete construction projects often include a clause that requires a minimum cement content to be used in concrete mixtures (Obla and Lobo 2015).