Title: Concrete Q&A: Lateral Pressure of Concrete in Formwork

Author(s):

Publication: Concrete International

Volume: 40

Issue: 6

Appears on pages(s): 60

Keywords:

DOI: 10.14359/51706902

Date: 6/1/2018

Abstract:
Q. I have been designing formwork for over 40 years and have several questions/comments regarding Eq. 4.2.2.1a(c) in ACI 347R-14.1 Why was this equation introduced and how was it developed? What is the significance of the 14 ft wall height in Table 4.2.2.1a(a)?

Related References:

1. ACI Committee 347, “Guide to Formwork for Concrete (ACI 347R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 36 pp.

2. ACI Committee 347, “Recommended Practice for Concrete Formwork (ACI 347-63),” American Concrete Institute, Farmington Hills, MI, 1963, 52 pp.

3. ACI Committee 662, “Pressures on Formwork,” ACI Journal Proceedings, V. 55, No. 8, Aug. 1958, pp. 173-190.

4. ACI Committee 347, “Guide to Formwork for Concrete (ACI 347R-94),” American Concrete Institute, Farmington Hills, MI, 1994, 34 pp.

5. ACI Committee 347, “Guide to Formwork for Concrete (ACI 347-01),” American Concrete Institute, Farmington Hills, MI, 2001, 32 pp.

6. ACI Committee 347, “Guide to Formwork for Concrete (ACI 347R-03),” American Concrete Institute, Farmington Hills, MI, 2003, 32 pp.

7. ACI Committee 347, “Guide to Formwork for Concrete (ACI 347-04),” American Concrete Institute, Farmington Hills, MI, 2004, 32 pp.