Insights on Pile Cap Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Insights on Pile Cap Construction

Author(s): Tadeusz Granosik and Guy Michel Chovelon

Publication: Concrete International

Volume: 40

Issue: 6

Appears on pages(s): 38-39

Keywords: casing, form, contractor, shaft

DOI: 10.14359/51706897

Date: 6/1/2018

Abstract:
An alternative method for construction of pile caps on single, bored cast-in-place piles is proposed. The method allows a single subcontractor to install both the pile and the pile cap, thereby saving time by eliminating the need for separate excavation, construction, and backfilling operations to complete the pile cap.