Modeling of Compressive Strength Development of High-Early-Strength-Concrete at Different Curing Temperatures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Modeling of Compressive Strength Development of High-Early-Strength-Concrete at Different Curing Temperatures

Author(s): Chadon Lee, Songhee Lee, and Ngocchien Nguyen

Publication: IJCSM

Volume: 10

Issue: 2

Appears on pages(s): 205–219

Keywords: high-early-strength concrete, compressive strength, curing temperature.

DOI: 10.1007/s40069-016-0147-6

Date: 6/30/2016

Abstract:
High-early-strength-concrete (HESC) made of Type III cement reaches approximately 50–70 % of its design compressivestrength in a day in ambient conditions. Experimental investigations were made in this study to observe the effects oftemperature, curing time and concrete strength on the accelerated development of compressive strength in HESC. A total of 210HESC cylinders of 100 9 200 mm were tested for different compressive strengths (30, 40 and 50 MPa) and different curingregimes (with maximum temperatures of 20, 30, 40, 50 and 60 C) at different equivalent ages (9, 12, 18, 24, 36, 100 and 168 h). From a series of regression analyses, a generalized rate-constant model was presented for the prediction of the compressivestrength of HESC at an early age for its future application in precast prestressed units with savings in steam supply. The averageand standard deviation of the ratios of the predictions to the test results were 0.97 and 0.22, respectively.