Experimental and Analytical Studies of U-Shaped Thin-Walled RC Beams Under Combined Actions of Torsion, Flexure and Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental and Analytical Studies of U-Shaped Thin-Walled RC Beams Under Combined Actions of Torsion, Flexure and Shear

Author(s): Jianchao Xu, Shenggang Chen, Quanquan Guo, Yinghua Ye, Bo Diao, and Y. L. Mo

Publication: IJCSM

Volume: 12

Issue:

Appears on pages(s):

Keywords: reinforced concrete, U-shaped thin-walled beam, combined action of torsion and flexure, warping torsion, ultimate load.

DOI: 10.1186/s40069-018-0245-8

Date: 3/30/2018

Abstract:
U-shaped thin-walled concrete bridge beams usually suffer the combined actions of flexure, shear and torsion, but no research about the behavior of U-shaped thin-walled RC beams under combined actions has been reported in literature. Three large specimens of U-shaped thin-walled RC beams were tested under different torque–bending moment ratios (T–M ratios) of 1:5, 1:1 and 1:0 to investigate the mechanical responses such as crack patterns, reinforcement strains, failure modes and ductility. The testing results showed that ductile flexural failures occurred for all three of the U-shaped thin-walled beam specimens, although the combined shear effect of circulatory torque, warping torque and shear force increased as the T–M ratio increased from 1:5 via 1:1 to 1:0, reflected by diagonal cracks and stirrup strains. More specifically, basically symmetrical flexural failure was dominated by the bending moment when the T–M ratio was 1:5; flexural failure of the loaded half of the U-shaped thin-walled section was dominated by the combined action of the bending moment and warping moment, while there were only a few cracks on the other half of the U-shaped section when the T–M ratio was 1:1; and anti-symmetrical flexural failure was dominated by the warping moment when the T–M ratio was 1:0 (pure torsion). A simple method to calculate the ultimate load of such U-shaped thin-walled RC beams under different T–M ratios was suggested, and the calculating results were corresponding well with the experimental results.