High Magnitude Loading of Concrete Bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High Magnitude Loading of Concrete Bridges

Author(s): Jacob W. Schmidt, Philip S. Halding, Thomas W. Jensen, Svend Engelund

Publication: Symposium Paper

Volume: 323

Issue:

Appears on pages(s): 9.1-9.20

Keywords: Full-scale testing, concrete bridges, test rig, advanced monitoring, Danish standard vehicles, structural response, modelling

DOI: 10.14359/51702439

Date: 5/1/2018

Abstract:
The motivation for full-scale testing of concrete bridges is significant, since it is deemed to solve some of the major challenges related to capacity evaluation of older concrete bridges combined with increasing load demands. A novel test rig was developed as a mean to evaluate the full-scale bridge response of concrete bridges spanning up to 12 m (39.4 feet). The test rig was fast to mount, applied the load accurately, and loaded the structures to a very high load magnitude. The bridges were loaded to maximum capacity of the test rig without cracking (approx. 100 tonne (220,000 lbs) axle loads). 3D scanning, LVDTs, distance lasers, and DIC cameras were applied to two of the bridges, as well as land surveying readings, in order to measure the structural behaviour during testing. The loading sequence worked well, and it was possible to measure deflections and strains. Using a wide-angle lens DIC-camera showed to be a promising method to measure strains, in-plane deformations and cracking during testing. Work regarding modelling in conjunction with monitoring is ongoing, to provide a more accurate way to evaluate the ultimate capacity of the bridges as well as stop criteria during full-scale testing.