Assessment of Slab Bridges through Proof Loading in The Netherlands

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessment of Slab Bridges through Proof Loading in The Netherlands

Author(s): Eva O. L. Lantsoght, Cor van der Veen, Ane de Boer and Dick A. Hordijk

Publication: Symposium Paper

Volume: 323

Issue:

Appears on pages(s): 1.1-1.20

Keywords: field testing; flexure; measurements; proof load testing; reinforced concrete; shear; slab bridges

DOI: 10.14359/51702431

Date: 5/1/2018

Abstract:
A large subset of the Dutch bridge stock consists of reinforced concrete slab bridges, for which assessment often results in low ratings. To prioritize the efforts of the bridge owner, more suitable assessment methods for slab bridges are necessary. Research efforts over the past years resulted in the development of several methods, at levels requiring increasing costs, time, and effort for increasing accuracy. The last option, when an analytical assessment is not possible due to uncertainties, is to use proof load testing to evaluate the bridge directly. To develop recommendations for the proof load testing of reinforced concrete slab bridges for the Netherlands, different methods are combined: pilot proof load tests on bridges with and without material damage, a collapse test, tests on beams taken from an existing bridge and new beams with similar dimensions cast in the laboratory, and an extensive literature review. The result of this study is a set of recommendations that describe how to prepare and execute a proof load test, and how to analyze the results. This paper summarizes the research program about proof load testing from the Netherlands and gives an overview of the currently developed recommendations and topics for further research.

Related References:

AASHTO, 2016, "The manual for bridge evaluation with 2016 interim revisions," 2nd ed. American Association of State Highway and Transportation Officials; Washington, D.C.

ACI Committee 437, 2013, "Code Requirements for Load Testing of Existing Concrete Structures (ACI 437.2M-13) and Commentary ", Farmington Hills, MA, 24 pp.

Aguilar, C. V., Jáuregui, D. V., Newtson, C. M., Weldon, B. D. and Cortez, T. M., 2015, "Load Rating a Prestressed Concrete Double-Tee Beam Bridge without Plans by Proof Testing," Transportation Research Board Annual Compendium of Papers, Washington DC, pp. 19.

Anay, R., Cortez, T. M., Jáuregui, D. V., ElBatanouny, M. K. and Ziehl, P., 2016, "On-Site Acoustic-Emission Monitoring for Assessment of a Prestressed Concrete Double-Tee-Beam Bridge without Plans," Journal of Performance of Constructed Facilities, V. 30, No. 4.

Arangjelovski, T., Gramatikov, K. and Docevska, M., 2015, "Assessment of damaged timber structures using proof load test – Experience from case studies," Construction and Building Materials, V. 101, Part 2, 12/30/, pp. 1271-1277.

Barker, M. G., 2001, "Quantifying Field-Test Behavior for Rating Steel Girder Bridges," Journal of Bridge Engineering, V. 6, No. 4, pp. 254-261.

Belletti, B., Hendriks, M. A. N., den Uijl, J. A. and Damoni, C., 2010, "Developing standardized guidelines for safety assessment of shear-critical rc beams based on nonlinear finite element modeling," 3rd fib International Congress, Washington DC, pp. 13.

Belletti, B., Damoni, c., Hendriks, M. A. N. and Den Uijl, J. A., 2013, "Nonlinear finite element analyses of reinforced concrete slabs: comparison of safety formats," VIII International Conference on Fracture Mecahnics of concrete and Concrete Structures, FraMCoS-8, Van Mier, J. G. M., Ruiz, G., Andrade, C., Yu, R. C. and Zhang, X. X., eds., pp. 12.

Belletti, B., Pimentel, M., Scolari, M. and Walraven, J. C., 2015, "Safety assessment of punching shear failure according to the level of approximation approach," Structural Concrete, V. 16, No. 3, pp. 366-380.

Bretschneider, N., Fiedler, L., Kapphahn, G. and Slowik, V., 2012, "Technical possibilities for load tests of concrete and masonry bridges," Bautechnik, V. 89, No. 2, pp. 102-110 (in German).

Bridge Diagnostics Inc., 2012, "Integrated Approach to Load Testing," 44 pp.

Casas, J. R. and Gómez, J. D., 2013, "Load Rating of Highway Bridges by Proof-loading," KSCE Journal of Civil Engineering, V. 17, No. 3, pp. 556-567.

CEN, 2002, "Eurocode – Basis of structural design, NEN-EN 1990:2002 ", Comité Européen de Normalisation, Brussels, Belgium, 103 pp.

CEN, 2003, "Eurocode 1: Actions on structures - Part 2: Traffic loads on bridges, NEN-EN 1991-2:2003," Comité Européen de Normalisation, Brussels, Belgium, 168 pp.

CEN, 2005, "Eurocode 2: Design of Concrete Structures - Part 1-1 General Rules and Rules for Buildings. NEN-EN 1992-1-1:2005," Comité Européen de Normalisation, Brussels, Belgium, 229 pp.

Cochet, D., Corfdir, P., Delfosse, G., Jaffre, Y., Kretz, T., Lacoste, G., Lefaucheur, D., Khac, V. L. and Prat, M., 2004, "Load tests on highway bridges and pedestrian bridges (in French)," Setra - Service d'Etudes techniques des routes et autoroutes, Bagneux-Cedex, France.

Code Committee 351001, 1995, "NEN 6720 Technical Foundations for Building Codes, Concrete provisions TGB 1990 - Structural requirements and calculation methods (VBC 1995) (in Dutch)," Civil engineering center for research and regulation, Dutch Normalization Institute, Delft, The Netherlands, 245 pp.

Cope, R. J., 1985, "Flexural Shear Failure of Reinforced-Concrete Slab Bridges," Proceedings of the Institution of Civil Engineers Part 2-Research and Theory, V. 79, No. SEP, pp. 559-583.

den Uijl, J. A. and Kaptijn, N., 2004, "Structural consequences of ASR: an example on shear capacity," Heron, V. 47, No. 2, pp. 1-13.

Deutscher Ausschuss für Stahlbeton, 2000, "DAfStb-Guideline: Load tests on concrete structures (in German)," Deutscher Ausschuss fur Stahlbeton, 7 pp.

Dieteren, G. G. A. and den Uijl, J. A., 2009, "Evaluation proof load test Heidijk (in Dutch)," V. 2008-DWARS-MOlO, TNO Bouw en Ondergrond / TU Delft, 70 pp.

Faber, M. H., Val, D. V. and Stewart, M. G., 2000, "Proof load testing for bridge assessment and upgrading," Engineering Structures, V. 22, pp. 1677-1689.

Fennis, S. A. A. M. and Hordijk, D. A., 2014, "Proof loading Halvemaans Bridge Alkmaar (in Dutch)," Stevin Report 25.5-14-05, Delft University of Technology, Delft, The Netherlands, 72 pp.

Fennis, S. A. A. M., van Hemert, P., Hordijk, D. and de Boer, A., 2014, "Proof loading Vlijmen-Oost; Research on assessment method for existing structures (in Dutch)," Cement, V. 5, pp. 40-45.

fib, 2012, "Model code 2010: final draft," International Federation for Structural Concrete; Lausanne, 676 pp.

Frýba, L. and Pirner, M., 2001, "Load tests and modal analysis of bridges," Engineering Structures, V. 23, No. 1, pp. 102-109.

Fu, G., Pezze III, F. P. and Alampalli, S., 1997, "Diagnostic Load Testing for Bridge Load Rating," Transportation Research Record, V. 1594, pp. 125-133.

JCSS, 2001, "JCSS Probabilistic Model Code - Part 3: Resistance Models".

Koekkoek, R. T., Lantsoght, E. O. L. and Hordijk, D. A., 2015, "Proof loading of the ASR-affected viaduct Zijlweg over highway A59," Stevin Report nr. 25.5-15-08, Delft University of Technology, Delft, The Netherlands, 180 pp.

Koekkoek, R. T., Lantsoght, E. O. L., Yang, Y. and Hordijk, D. A., 2016, "Analysis report for the assessment of Viaduct De Beek by Proof Loading," Stevin Report 25.5-16-01, Delft University of Technology, Delft, The Netherlands, 125 pp.

Lantsoght, E., 2016, "Literature review on load testing," Stevin Report nr. 25.5-16-07, Delft University of Technology, 102 pp.

Lantsoght, E., van der Veen, C. and de Boer, A., 2016a, "Shear and moment capacity of the Ruytenschildt bridge," IABMAS 2016, pp. 8.

Lantsoght, E., Yang, Y., van der Veen, C., de Boer, A. and Hordijk, D., 2016b, "Ruytenschildt Bridge: field and laboratory testing," Engineering Structures, V. 128, No. december, pp. 111-123.

Lantsoght, E., 2017a, "Measurements of Ruytenschildt Bridge test and analysis for stop criteria," V. Stevin Report nr. 25.5-17-02, Delft University of Technology, 60 pp.

Lantsoght, E., 2017b, "Development of a stop criterion for shear based on aggergate interlock," V. Stevin Report nr. 25.5-17-09, Delft University of Technology, 33 pp.

Lantsoght, E. O. L., de Boer, A., Van der Veen, C. and Walraven, J. C., 2013a, "Peak shear stress distribution in finite element models of concrete slabs," Research and Applications in Structural Engineering, Mechanics and Computation, Zingoni, A., ed. Cape Town, South Africa, pp. 475-480.

Lantsoght, E. O. L., van der Veen, C., de Boer, A. and Walraven, J. C., 2013b, "Recommendations for the Shear Assessment of Reinforced Concrete Slab Bridges from Experiments " Structural Engineering International, V. 23, No. 4, pp. 418-426.

Lantsoght, E. O. L., van der Veen, C. and Walraven, J. C., 2013c, "Shear in One-way Slabs under a Concentrated Load close to the support," ACI Structural Journal, V. 110, No. 2, pp. 275-284.

Lantsoght, E. O. L., De Boer, A. and van der Veen, C., 2014a, "Determination of distribution width for shear stresses at support in reinforced concrete slab bridges," EuroC, St. Anton am Arlberg, Austria, pp. 9

Lantsoght, E. O. L., van der Veen, C., De Boer, A. and Walraven, J., 2014b, "Influence of Width on Shear Capacity of Reinforced Concrete Members," ACI Structural Journal, V. 111, No. 6, pp. 1441-1450.

Lantsoght, E. O. L., van der Veen, C., de Boer, A. and Walraven, J., 2015a, "One-way slabs subjected to combination of loads failing in shear," ACI Structural Journal, V. 112, No. 4, pp. 417-426.

Lantsoght, E. O. L., Van der Veen, C., de Boer, A. and Walraven, J. C., 2015b, "Proposal for the extension of the Eurocode shear formula for one-way slabs under concentrated loads," Engineering Structures, V. 95, pp. 16-24.

Lantsoght, E. O. L., van der Veen, C., Walraven, J. and de Boer, A., 2015c, "Experimental investigation on shear capacity of reinforced concrete slabs with plain bars and slabs on elastomeric bearings," Engineering Structures, V. 103, pp. 1-14.

Lantsoght, E. O. L., van der Veen, C. and de Boer, A., 2016c, "Shear capacity of the Rutyenschildt Bridge," fib Symposium 2016, Performance-based approaches for concrete structures, Beushausen, H., ed. Cape Town, South Africa, pp. 10.

Lantsoght, E. O. L., van der Veen, C., de Boer, A. and Alexander, S., 2016d, "Bridging the gap between one-way and two-way shear in slabs," ACI SP International Punching Symposium, pp. 20.

Lantsoght, E. O. L., van der Veen, C., de Boer, A. and Hordijk, D. A., 2016e, "Probabilistic prediction of the failure mode of the Ruytenschildt Bridge," Engineering Structures, V. 127, 11/15/, pp. 549-558.

Lantsoght, E. O. L., van der Veen, C., de Boer, A. and Walraven, J., 2016f, "Using Eurocodes and AASHTO for assessing shear in slab bridges," Proceedings of the Institution of Civil Engineers – Bridge Engineering, V. 169, No. BE4, pp. 285-297.

Lantsoght, E. O. L., Yang, Y., Tersteeg, R. H. D., van der Veen, C. and de Boer, A., 2016g, "Development of Stop Criteria for Proof Loading," IALCCE 2016, Delft, The Netherlands, pp. 8 pp.

Lantsoght, E. O. L., 2017c, "Beams from Ruytenschildt Bridge: Analysis of stop criteria," Stevin Report 25.5-17-05, Delft University of Technology, 77 pp.

Lantsoght, E. O. L., De Boer, A. and Van der Veen , C., 2017a, "Levels of Approximation for the shear assessment of reinforced concrete slab bridges," Structural Concrete, V. 18, pp. 143-152.

Lantsoght, E. O. L., Koekkoek, R. T., Hordijk, D. A. and De Boer, A., 2017b, "Towards standardization of proof load testing: pilot test on viaduct Zijlweg," Structure and Infrastructure Engineering.

Lantsoght, E. O. L., van der Veen, C. and de Boer, A., 2017c, "Extended Strip Model for slabs subjected to load combinations," Engineering Structures, V. 145, pp. 60-69.

Lantsoght, E. O. L., van der Veen, C., de Boer, A. and Alexander, S. D. B., 2017d, "Extended Strip Model for Slabs under Concentrated Loads," ACI Structural Journal, V. 114, No. 2, pp. 565-574.

Lantsoght, E. O. L., Van der Veen , C., De Boer, A. and Hordijk, D. A., 2017e, "Collapse test and moment capacity of the Ruytenschildt Reinforced Concrete Slab Bridge " Structure and Infrastructure Engineering, V. 13, No. 9, pp. 1130-1145.

Lantsoght, E. O. L., van der Veen, C., Hordijk, D. A. and de Boer, A., 2017f, "Reliability index after proof load testing: viaduct De Beek," ESREL 2017, Protoroz, Slovenia, pp. 8.

Lantsoght, E. O. L., Yang, Y., van der Veen, C., de Boer, A. and Hordijk, D. A., 2017g, "Beam experiments on acceptance criteria for bridge load tests," ACI Structural Journal, V. 114, No. 4, pp. 1031-1041.

Lantsoght, E. O. L., van der Veen, C., Hordijk, D. A. and de Boer, A., 2017h, "State-of-the-art on load testing of concrete bridges," Engineering Structures, V. 150, pp. 231-241.

Lantsoght, E. O. L., Koekkoek, R. T., van der Veen, C., Hordijk, D. A. and de Boer, A., in press-a, "Case study: Pilot proof load test on viaduct De Beek," Journal of Bridge Engineering.

Lantsoght, E. O. L., Van der Veen , C., De Boer, A. and Hordijk, D. A., in press-b, "Proof load testing of reinforced concrete slab bridges in the Netherlands," Structural Concrete, pp. 29.

Matta, F., Bastianini, F., Galati, N., Casadei, P. and Nanni, A., 2008, "Distributed Strain Measurement in Steel Bridge with Fiber Optic Sensors: Validation through Diagnostic Load Test," Journal of Performance of Constructed Facilities, V. 22, No. 4, pp. 264-273.

Moses, F., Lebet, J. P. and Bez, R., 1994, "Applications of field testing to bridge evaluation," Journal of Structural Engineering-ASCE, V. 120, No. 6, Jun, pp. 1745-1762.

Olaszek, P., Swit, G. and Casas, J. R., 2012, "Proof load testing supported by acoustic emission. An example of application," IABMAS 2012.

Olaszek, P., Lagoda, M. and Casas, J. R., 2014, "Diagnostic load testing and assessment of existing bridges: examples of application," Structure and Infrastructure Engineering, V. 10, No. 6, Jun 3, pp. 834-842.

PN-S-10040/99, 1999, "Bridges. Concrete, reinforced concrete and prestressed structures. Requirements and testing. (in Polish)."

Rijkswaterstaat, 2013, "Guidelines Assessment Bridges - assessment of structural safety of an existing bridge at reconstruction, usage and disapproval (in Dutch), RTD 1006:2013 1.1," 117 pp.

Rijkswaterstaat, 2014, "Guidelines for coring, transporting, and testing of concrete cores and the determination of the compressive and splitting tensile strength (in Dutch)," RTD 1021:2014, Rijkswaterstaat, 29 pp.

Rijkswaterstaat, 2016, "Guidelines for Nonlinear Finite Element Analysis of Concrete Structures," RTD 1016:2012, 65 pp.

Russo, F. M., Wipf, T. J. and Klaiber, F. W., 2000, "Diagnostic Load Tests of a Prestressed Concrete Bridge Damaged by Overheight Vehicle Impact," Transportation Research Record, V. 1696, pp. 103-110.

Sanayei, M., Reiff, A. J., Brenner, B. R. and Imbaro, G. R., 2016, "Load Rating of a Fully Instrumented Bridge: Comparison of LRFR Approaches," Journal of Performance of Constructed Facilities, V. 2016, No. 30, pp. 2.

Saraf, V. K., Nowak, A. S. and Till, R., 1996, "Proof load testing of bridges," Probabilistic Mechanics & Structural Reliability: Proceedings of the Seventh Specialty Conference, Frangopol, D. M. and Grigoriu, M. D., eds., Worcester, MA, USA, pp. 526-529.

Stewart, M. G. and Val, D. V., 1999, "Role of load history in reliability-based decision analysis of aging bridges," Journal of Structural Engineering-ASCE, V. 125, No. 7, pp. 776-783.

Velázquez, B. M., Yura, J. A., Frank, K. H., Kreger, M. E. and Wood, S. L., 2000, "Diagnostic load tests of a reinforced concrete pan-girder bridge," V. Research Report 7-2986-2, The University of Texas at Austin, Austin, TX, USA, 121 pp.

Vergoossen, R., Naaktgeboren, M., ‘t Hart, M., De Boer, A. and Van Vugt, E., 2013, "Quick Scan on Shear in Existing Slab Type Viaducts," International IABSE Conference, Assessment, Upgrading and Refurbishment of Infrastructures, Rotterdam, The Netherlands, pp. 8.

Vrouwenvelder, T., Holicky, M. and Markova, J., 2002, "JCSS Probabilistic Model Code Example Applications," 19 pp.

Yang, Y., 2015, "Experimental Studies on the Structural Behaviours of Beams from Ruytenschildt Bridge," Stevin Report 25.5-15-09, Delft University of Technology, Delft, 76 pp.

Yang, Y., Den Uijl, J. A. and Walraven, J., 2016 "The Critical Shear Displacement theory: on the way to extending the scope of shear design and assessment for members without shear reinforcement," Structural Concrete, V. 17, No. 5, pp. 790-798.

Yang, Y., Walraven, J. and den Uijl, J. A., 2017, "Shear Behavior of Reinforced Concrete Beams without Transverse Reinforcement Based on Critical Shear Displacement," Journal of Structural Engineering, V. 143, No. 1.