Minimum Shear Reinforcement of Slender Walls with Grade 500 MPa (72.5 ksi) Reinforcing Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Minimum Shear Reinforcement of Slender Walls with Grade 500 MPa (72.5 ksi) Reinforcing Bars

Author(s): Jang-Woon Baek, Hong-Gun Park, Kyung-Kyu Choi, Min-Seok Seo, and Lan Chung

Publication: Structural Journal

Volume: 115

Issue: 3

Appears on pages(s): 761-774

Keywords: cyclic loading; high-strength reinforcing bars; low reinforcing bar ratio; minimum shear reinforcement; slender walls

DOI: 10.14359/51701281

Date: 5/1/2018

Abstract:
For the shear design of reinforced concrete (RC) walls, ACI 318 requires minimum shear reinforcement ratio in the case of 0.5ϕVc ≤ Vu < ϕVc, and the yield strength of shear reinforcement is limited to 420 MPa (60 ksi). In this study, to investigate the effect of Grade 500 MPa (72.5 ksi) reinforcing bars on the shear strength and minimum shear reinforcement of RC walls, slender walls (aspect ratio of 2.5) with Grade 500 MPa (72.5 ksi) shear reinforcement were tested under cyclic lateral loading. The test parameters included the failure modes, the grade and ratio of shear reinforcement, concrete compressive strength, and axial compression. The test results of walls with 500 MPa (72.5 ksi) reinforcing bars were directly compared with those of walls with 400 MPa (58 ksi) reinforcing bars. Further, the test strengths were compared with the predictions by current design codes.

Related References:

1. British Standards Institution, “Eurocode 2: Design of Concrete Structures – Part 1-1: General Rules and Rules for Building,” European Standard EN-1992-1-1:2004:E, European Committee for Standardization, Brussels, Belgium, 2004, 225 pp.

2. Canadian Standards Association, “Design of Concrete Structures,” Canadian Standards Association, Rexdale, ON, Canada, 2004, 214 pp.

3. Japan Society of Civil Engineers, “Standard Specifications for Concrete Structures–2007: Design,” Japan Society of Civil Engineers, Tokyo, Japan, 2010, 469 pp.

4. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

5. Cardenas, A. E.; Hanson, J. M.; Corley, W. G.; and Hognestad, E., “Design Provisions for Shear Walls,” ACI Journal Proceedings, V. 70, No. 3, Mar. 1973, pp. 221-230.

6. Barda, F.; Hanson, J. M.; and Corley, W. G., “Shear Strength of Low-Rise Walls with Boundary Elements,” Reinforced Concrete Structures in Seismic Zones, SP-53, N. M. Hawkins and D. Mitchell, eds., American Concrete Institute, Farmington Hills, MI, 1977, pp. 149-202.

7. Hidalgo, P. A.; Ledezma, C. A.; and Jordan, R. M., “Seismic Behavior of Squat Reinforced Concrete Shear Walls,” Earthquake Spectra, V. 18, No. 2, 2002, pp. 287-308. doi: 10.1193/1.1490353

8. Carrillo, J., and Alcocer, S. M., “Seismic Performance of Concrete Walls for Housing subjected to Shaking Table Excitations,” Engineering Structures, V. 41, 2012, pp. 98-107. doi: 10.1016/j.engstruct.2012.03.025

9. Sánchez, A., “Seismic Behavior of Housing with Concrete Walls,” Technical Report, Institute of Engineering, Universidad Nacional Autonoma de Mexico, Mexico City, Mexico, 2010, 475 pp.

10. Carrillo, J., and Alcocer, S., “Shear Strength of Reinforced Concrete Walls for Seismic Design of Low-Rise Housing,” ACI Structural Journal, V. 110, No. 3, May-June 2013, pp. 415-425.

11. Hirosawa, M., “Past Experimental Results on Reinforced Concrete Shear Walls and Analysis on Them (in Japanese),” Building Research Institute, Ministry of Construction, Tokyo, Japan, 1975, 273 pp.

12. Gao, X., “Framed Shear Walls under Cyclic Loading,” PhD thesis, Department of Civil and Environmental Engineering, University of Houston, Houston, TX, 1999, 285 pp.

13. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

14. Pilakoutas, K., and Elnashiai, A., “Cyclic Behavior of Reinforced Concrete Cantilever Walls, Part 1: Experimental Results,” ACI Structural Journal, V. 92, No. 3, May-June, 1995, pp. 271-281.

15. Park, R., “Ductility Evaluation from Laboratory and Analytical Testing,” Proceedings of the 9th World Conference on Earthquake Engineering, 1988, Tokyo-Kyoto, Japan, pp. 605-616.

16. Baek, J. W.; Park, H. G.; Shin, H. M.; and Yim, S. J., “Cyclic Loading Test for Reinforced Concrete Walls (Aspect Ratio 2.0) with Grade 550 MPa (80 ksi) Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 3, May-June 2017, pp. 673-686. doi: 10.14359/51689437

17. Baek, J. W.; Park, H. G.; Lee, J. H.; and Bang, C. J., “Cyclic Loading Test for Walls of Aspect Ratio 1.0 and 0.5 with Grade 550 MPa (80 ksi) Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 4, July-Aug. 2017, pp. 969-982. doi: 10.14359/51689680

18. Wood, S. L., “Shear Strength of Low-Rise Reinforced Concrete Walls,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 99-107.

19. Gulec, C. K., and Whittaker, A. S., “Empirical Equations for Peak Shear Strength of Low Aspect Ratio Reinforced Concrete Walls,” ACI Structural Journal, V. 108, No. 1, Jan.-Feb. 2011, pp. 80-89.

20. Greifenhagen, C., and Lestuzzi, P., “Static Cyclic Tests on Lightly Reinforced Concrete Shear Walls,” Engineering Structures, V. 27, No. 11, 2005, pp. 1703-1712. doi: 10.1016/j.engstruct.2005.06.008

21. Massone, L. M., and Wallace, J. W., “Load-Deformation Responses of Slender Reinforced Concrete Walls,” ACI Structural Journal, V. 101, No. 1, Jan.-Feb. 2004, pp. 103-113.

22. Park, H. G.; Baek, J. W.; Lee, J. H.; and Shin, H. M., “Cyclic Loading Tests for Shear Strength of Low-Rise Reinforced Concrete Walls with Grade 550 MPa Bars,” ACI Structural Journal, V. 112, No. 3, May-June 2015, pp. 299-310. doi: 10.14359/51687406


ALSO AVAILABLE IN:

Electronic Structural Journal