Experimental Investigation of Thin-Wall Synthetic Fiber-Reinforced Concrete Pipes

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Investigation of Thin-Wall Synthetic Fiber-Reinforced Concrete Pipes

Author(s): Fouad T. Al Rikabi, Shad M. Sargand, John Kurdziel, and Husam H. Hussein

Publication: Structural Journal

Volume: 115

Issue: 6

Appears on pages(s): 1671-1681

Keywords: composite materials; concrete pipes; fiber-reinforced concrete; sewers; synthetic fiber

DOI: 10.14359/51702413

Date: 11/1/2018

Abstract:
Synthetic fibers have been recently used to enhance the ductility, durability, flexural strength, and shear strength of concrete pipes while reducing the steel reinforcement. However, using the same pipe wall thickness specified by ASTM standards did not result in a significant enhancement in the flexibility of fiber-reinforced concrete pipe. This research investigates the effect on the flexibility, strength, stiffness, and strain capacity of using minimal steel reinforcement with the polypropylene fiber-reinforced concrete pipe with reduced wall thickness. Concrete pipes with diameters of 1200 and 1500 mm (48 and 60 in.) with respective wall thicknesses of 50 and 63 mm (2 and 2.5 in.) were tested under a three-edge bearing load. To assure maximum fiber contribution to pipe strength, a 9 kg/m3 (15 lb/yd3) fiber dosage was used with different amounts of steel reinforcement. Results showed that all tested pipes surpassed 5% deflection of their inside diameter with high load capacity. The tested pipes exhibited flexural failure, and at higher loading levels, radial and shear failure modes were also observed. Concrete pipe with a diameter of 1200 mm (48 in.) reinforced with steel area of 10.2 cm2/m (0.48 in.2/ft) fulfilled the ultimate strength requirements of ASTM for Classes I, II, and III. Also, concrete pipe with a diameter of 1500 mm (60 in.) reinforced with a steel area of 8.9 cm2/m (0.42 in.2/ft) did not fulfill the ultimate strength requirements of ASTM for Classes I and II. These pipes exhibited stiffnesses as high as 7.8 and 10.2 times that of high-density polyethylene pipe at 5% deflection for diameters of 1200 and 1500 mm (48 and 60 in.), respectively. Increasing steel area also increased the strain capacity of the pipes. Also, comparing with past research, increasing fiber dosage from 4.75 to 9 kg/m3 (8 to 15 lb/yd3) increased the stiffness by 95%.

Related References:

AASHTO, 2011, “Standard Specification for Corrugated Polyethylene Pipe, 300- to 1500-mm (12- to 60-in.) Diameter,” M 294-11, Washington, DC.

Al Rikabi, F.; Sargand, S.; and Kurdziel, J., 2019, “Evaluation of Synthetic Fiber Reinforced Concrete Pipe Performance Using Three-Edge Bearing Test,” Journal of Testing and Evaluation, V. 47, No. 2, p. 20170369 doi: 10.1520/JTE20170369

Altoubat, S.; Yazdanbakhsh, A.; and Rieder, K. A., 2009, “Shear Behavior of Macrosynthetic Fiber-Reinforced Concrete Beams without Stirrups,” ACI Materials Journal, V. 106, No. 4, July-Aug., pp. 381-389.

ASCE, 2001, “Standard Practice for Direct Design of Precast Concrete Pipe Using Standard Installations (SIDD) (ASCE 15-98),” American Society of Civil Engineers, Reston, VA, 40 pp.

ASTM C76-15a, 2015, “Standard Specification for Reinforced Concrete Culvert, Storm Drain, and Sewer Pipe,” ASTM International, West Conshohocken, PA, 11 pp.

ASTM C497-15, 2015, “Standard Test Methods for Concrete Pipe, Manhole Sections, or Tile,” ASTM International, West Conshohocken, PA, 13 pp.

ASTM F2648/2648M-13, 2013, “Standard Specification for 2 to 60 inch [50 to 1500 mm] Annular Corrugated Profile Wall Polyethylene (PE) Pipe and Fittings for Land Drainage Applications,” ASTM International, West Conshohocken, PA, 8 pp.

Balaguru, P., and Shah, S., 1992, Fiber-Reinforced Cement Composites, McGraw-Hill Inc., New York.

Banthia, N., and Dubey, A., 2000, “Measurement of Flexural Toughness of Fiber-Reinforced Concrete Using a Novel Technique—Part 2: Performance of Various Composites,” ACI Materials Journal, V. 97, No. 1, Jan.-Feb., pp. 3-11.

Çavdar, A., 2012, “A Study on the Effects of High Temperature on Mechanical Properties of Fiber Reinforced Cementitious Composites,” Composites. Part B, Engineering, V. 43, No. 5, pp. 2452-2463. doi: 10.1016/j.compositesb.2011.10.005

Çavdar, A., 2013, “The Effects of High Temperature on Mechanical Properties of Cementitious Composites Reinforced with Polymeric Fibers,” Composites. Part B, Engineering, V. 45, No. 1, pp. 78-88. doi: 10.1016/j.compositesb.2012.09.033

Çavdar, A., 2014, “Investigation of Freeze-Thaw Effects on Mechanical Properties of Fiber Reinforced Cement Mortars,” Composites. Part B, Engineering, V. 58, pp. 463-472. doi: 10.1016/j.compositesb.2013.11.013

de la Fuente, A.; Escariz, R. C.; de Figueiredo, A. D.; and Aguado, A., 2013, “Design of Macro-Synthetic Fibre Reinforced Concrete Pipes,” Construction and Building Materials, V. 43, pp. 523-532. doi: 10.1016/j.conbuildmat.2013.02.036

Gabriel, L. H., 2011, Corrugated Polyethylene Pipe Design Manual and Installation Guide, Plastic Pipe Institute, Irving, TX.

Heger, F. J., 1963, “Structural Behavior of Circular Reinforced Concrete Pipe—Development of Theory,” ACI Journal Proceedings, V. 60, No. 11, Nov., pp. 1567-1614.

Heger, F. J., and Gillespie, J. W., 1967, “Design of Circular Concrete Pipe Reinforced with Welded Deformed Wire Fabric,” No. HS-000 708, sponsored by Committee on Culverts and Culvert Pipe.

Heger, F. J., and McGrath, T. J., 1983, “Radial Tension Strength of Pipe and Other Curved Flexural Members,” ACI Journal Proceedings, V. 80, No. 1, Jan., pp. 33-39.

Kani, G. N. J., 1964, “The Riddle of Shear Failure and its Solution,” ACI Journal Proceedings, V. 61, No. 4, Apr., pp. 441-468.

Kuder, K. G., and Shah, S. P., 2010, “Processing of High-Performance Fiber-Reinforced Cement-Based Composites,” Construction and Building Materials, V. 24, No. 2, pp. 181-186. doi: 10.1016/j.conbuildmat.2007.06.018

Li, V. C., and Maalej, M., 1996, “Toughening in Cement-Based Composites. Part II: Fiber Reinforced Cementitious Composites,” Cement and Concrete Composites, V. 18, No. 4, pp. 239-249. doi: 10.1016/0958-9465(95)00029-1

Mobasher, B., and Li, C. Y., 1996, “Mechanical Properties of Hybrid Cement-Based Composites,” ACI Materials Journal, V. 93, No. 3, May-June, pp. 284-292.

Park, Y.; Abolmaali, A.; Attiogbe, E.; and Lee, S. H., 2014, “Time-Dependent Behavior of Synthetic Fiber-Reinforced Concrete Pipes under Long-Term Sustained Loading,” Transportation Research Record: Journal of the Transportation Research Board, V. 2407, No. 1, pp. 71-79. doi: 10.3141/2407-07

Park, Y.; Abolmaali, A.; Beakley, J.; and Attiogbe, E., 2015, “Thin-Walled Flexible Concrete Pipes with Synthetic Fibers and Reduced Traditional Steel Cage,” Engineering Structures, V. 100, pp. 731-741. doi: 10.1016/j.engstruct.2015.06.049

Peyvandi, A.; Soroushian, P.; and Jahangirnejad, S., 2013, “Enhancement of the Structural Efficiency and Performance of Concrete Pipes through Fiber Reinforcement,” Construction and Building Materials, V. 45, pp. 36-44.

Peyvandi, A.; Soroushian, P.; and Jahangirnejad, S., 2014, “Structural Design Methodologies for Concrete Pipes with Steel and Synthetic Fiber Reinforcement,” ACI Structural Journal, V. 111, No. 1, Jan.-Feb., pp. 83-92.

Wilson, A., and Abolmaali, A., 2014, “Performance of Synthetic Fiber-Reinforced Concrete Pipes,” Journal of Pipeline Systems Engineering and Practice, V. 5, No. 3, Aug., pp. 1-10. doi: 10.1061/(ASCE)PS.1949-1204.0000166

Zollo, R. F., 1997, “Fiber-Reinforced Concrete: An Overview after 30 Years of Development,” Cement and Concrete Composites, V. 19, No. 2, pp. 107-122. doi: 10.1016/S0958-9465(96)00046-7


ALSO AVAILABLE IN:

Electronic Structural Journal