311.7-18: Inspection Services Specification for Cast-In-Place Concrete Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 311.7-18: Inspection Services Specification for Cast-In-Place Concrete Construction

Author(s): ACI Committee 311

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 8

Keywords: accreditation; certification; concrete construction; inspection agency; placement; post-placement; preplacement; special inspection; specification; 311; 311.7

DOI:

Date: 4/24/2018

Abstract:

This reference specification covers quality assurance inspection services for preplacement, placement, and post-placement of concrete construction. This reference specification can be made applicable to a particular construction project by citing it in the inspection services contract. The specifier shall supplement the provisions of this reference specification as needed by specifying individual project requirements in the inspection services contract.

The materials, processes, quality control measures, and inspections described in this specification should be tested, monitored, or performed as applicable only by individuals holding the appropriate ACI Certifications or equivalent.