An Innovative Approach to Concrete Mixture Proportioning

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Innovative Approach to Concrete Mixture Proportioning

Author(s): Xuhao Wang, Peter Taylor, Ezgi Yurdakul, and Xin Wang

Publication: Materials Journal

Volume: 115

Issue: 5

Appears on pages(s): 749-759

Keywords: aggregate system; mixture proportioning; optimization; paste quality; paste quantity; performance-based specifications; slipform pavement concrete

DOI: 10.14359/51702351

Date: 9/1/2018

Abstract:
Slipform paving is a road construction process where concrete is extruded by a paver that forms the stiff, fresh concrete into the desired slab shape. Slipform paving is especially suitable for time-sensitive projects requiring high productivity, as it allows placement of 65 to 100 m3 (85 to 130 yds) of concrete per hour. Mixture proportioning for slipform paving applications has often been based on recipes or previous mixtures rather than based on developing proportions for the specific needs of the project using local material. Therefore, a performance-based mixture proportioning approach is needed to balance the target performance requirements for workability, strength, durability, and cost effectiveness for a given project specification. The aim of this study was to develop an innovative performance based mixture proportioning method by analyzing the relationships between the selected mixture characteristics and their corresponding effects on concrete performance. The proposed method provides step-by-step instructions to guide the selection of required aggregate and paste systems based on the performance requirements of slipform pavements.

Related References:

1. Kosmatka, K., and Wilson, M. L., Design and Control of Concrete of Mixtures, 16th edition, Portland Cement Association, Skokie, IL, 2016.

2. Taylor, P.; Yurdakul, E.; Wang, X.; and Wang, X., “Concrete Pavement Mixture Design and Analysis (MDA): An Innovative Approach to Proportioning Concrete Mixtures,” Technical Report, National Concrete Pavement Technology Center, Iowa State University, Ames, IA, 2015, 40 pp.

3. Ozyildirim, C., “Virginia’s End-Result Specifications,” Concrete International, V. 33, No. 3, Mar. 2011, pp. 41-45.

4. Yurdakul, E.; Taylor, P.; Ceylan, H.; and Bektas, F., “Effects of Paste-to-Voids Volume Ratio on the Performance of Concrete Mixtures,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 12, 2013, pp. 1840-1851. doi: 10.1061/(ASCE)MT.1943-5533.0000728

5. Lee, B. Y.; Kim, J. H.; and Kim, J. K., “Optimum Concrete Mixture Proportion Based on a Database Considering Regional Characteristics,” Journal of Computing in Civil Engineering, ASCE, V. 23, No. 5, 2009, pp. 258-265. doi: 10.1061/(ASCE)0887-3801(2009)23:5(258)

6. Cook, M.; Ley, T.; and Ghaeezadah, A., “Effects of Aggregate Concepts on the Workability of Slip-Formed Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 10, 2016, 04016097. doi: 10.1061/(ASCE)MT.1943-5533.0001608

7. Li, C.; Ashlock, J.; Cetin, B.; Jahren, C.; and Goetz, V., “Performance-Based Design Method for Gradation and Plasticity of Granular Road Surface Materials,” Transportation Research Record: Journal of the Transportation Research Board, 2018. doi: 10.1177/0361198118787372.

8. Falker, E. M., “Assessing the Impact of Performance-Related Specifications on Concrete Pavement Construction,” MS thesis, Purdue University, West Lafayette, IN, 2003.

9. Hooton, R. D., and Bickley, J. A., “Prescriptive versus Performance Approaches for Durability Design—The End of Innocence?” Materials and Corrosion, V. 63, No. 12, 2012, pp. 1097-1101. doi: 10.1002/maco.201206780

10. Dhir, R. K.; McCarthy, M. J.; Zhou, S.; and Tittle, P. A. J., “Discussion: Role of Cement Content in Specifications for Concrete Durability: Aggregate Type Influences,” Structures and Buildings, V. 159, 2006, pp. 361-363.

11. Alexander, M., and Mindess, S., Aggregates in Concrete, Taylor & Francis, New York, 2005, 448 pp.

12. Kennedy, C., “The Design of Concrete Mixes,” ACI Journal Proceedings, V. 36, 1940, pp. 373-400.

13. Shilstone, J. M. Sr., and Shilstone, J. M. Jr., “Performance-Based Concrete Mixtures and Specifications Today,” Concrete International, V. 24, No. 2, Feb. 2002, pp. 80-83.

14. Cook, D.; Ghaeezadah, A.; and Ley, M. T., “A Workability Test for Slip Formed Concrete Pavements,” Construction and Building Materials, V. 68, 2014, pp. 376-383. doi: 10.1016/j.conbuildmat.2014.06.087

15. Ley, T. and Cook, D., “Aggregate Gradations for Concrete Pavement Mixtures,” Moving Advancements into Practice (MAP) Brief, FHWA TPF-5-(286), 2014, 4 pp., www.cproadmap.org/publications/MAPbriefOctober2014.pdf. (last accessed Sept. 19, 2018)

16. Taylor, P., “The Use of Ternary Mixtures in Concrete,” Technical Report, National Concrete Pavement Technology Center, Iowa State University, Ames, IA, 2014, 22 pp.

17. Mindess, S.; Young, J. F.; and Darwin, D., Concrete, second edition, Prentice Hall, Upper Saddle River, NJ, 2003, 644 pp.

18. AASHTO PP 84, “Standard Practice for Developing Performance Engineered Concrete Pavement Mixtures,” American Association of State and Highway Transportation Officials, Washington, DC, 2017, 77 pp.

19. Koehler, E., and Fowler, D., “ICAR Mixture Proportioning Procedure for Self-Consolidating Concrete,” Research Report ICAR 108-1, International Center for Aggregates Research, University of Texas at Austin, Austin, TX, 2006, 24 pp.

20. Wang, X.; Taylor, P.; Wang, K.; and Morcous, G., “Effects of Paste-to-Voids Volume Ratio on Performance of Self-Consolidating Concrete Mixtures,” Magazine of Concrete Research, V. 67, No. 14, 2015, pp. 771-785. doi: 10.1680/macr.14.00313

21. ASTM C29-16, “Standard Test Method for Bulk Density (Unit Weight) and Voids in Aggregate,” ASTM International, West Conshohocken, PA, 2016, 5 pp.

22. ASTM C150/C150M-17, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2017, 9 pp.

23. ASTM C618-15, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2015, 5 pp.

24. ASTM C231/C231-14, “Standard Test Method for Air Content of Freshly Mixed Concrete by the Pressure Method,” ASTM International, West Conshohocken, PA, 2014, 9 pp.

25. Taylor, P., and Wang, X., “Workability and Setting Time for Slipform Paving Concrete Mixtures,” Concrete International, V. 38, No. 8, Aug. 2016, pp. 41-48.

26. Wang, X.; Wang, K.; Taylor, P.; and Morcous, G., “Assessing Particle Packing Based Self-Consolidating Concrete Mix Design Method,” Construction and Building Materials, V. 70, 2014, pp. 439-452. doi: 10.1016/j.conbuildmat.2014.08.002

27. Taylor, P.; Bektas, F.; Yurdakul, E.; and Ceylan, H., “Optimizing Cementitious Content in Concrete Mixtures for Required Performance,” Technical Report, National Concrete Pavement Technology Center, Iowa State University, Ames, IA, 2012, 46 pp.

28. Taylor, P.; Yurdakul, E.; Ceylan, H.; and Bektas, F., “Development of Performance Properties of Ternary Mixtures and Concrete Pavement Mixture Design and Analysis (MDA): Effect of Paste Quality on Fresh and Hardened Properties of Ternary Mixtures,” Technical Report, National Concrete Pavement Technology Center, Iowa State University, Ames, IA, 2012, 45 pp.

29. Obla, K. H., “Optimizing Concrete Mixtures for Performance and Sustainability,” Proceedings of International Concrete Sustainability Conference, Seattle, WA, 2012.

30. Cook, D.; Ghaeezadeh, A.; Ley, T.; and Russell, B., “Investigation of Optimized Graded Concrete for Oklahoma – Phase I, Final Report,” ODOT SP&R Item Number 2160, State Planning and Research Division, Oklahoma Department of Transportation, Oklahoma City, OK, 2013.

31. ASTM C143/C143M-15, “Standard Test Method for Slump of Hydraulic Cement Concrete,” ASTM International, West Conshohocken, PA, 2015, 4 pp.

32. ASTM C1202-12, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2012, 8 pp.

33. ASTM C39/C39M-17, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens.” ASTM International, West Conshohocken, PA, 2017, 8 pp.

34. ASTM C157-08(2014), “Standard Test Method for Length Change of Hardened Hydraulic-Cement Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2014, 7 pp.

35. Hale, W. M.; Freyne, S. F.; Bush, T. D. Jr.; and Russell, B. W., “Properties of Concrete Mixtures Containing Slag Cement and Fly Ash for Use in Transportation Structures,” Construction and Building Materials, V. 22, No. 9, 2008, pp. 1990-2000. doi: 10.1016/j.conbuildmat.2007.07.004

36. Arachchige, A., “Influence of Cement Content on Corrosion Resistance,” Proceedings of the ICE – Construction Materials, V. 161, 2008, pp. 31-39.

37. AASHTO TP 95, “Standard Method of Test for Surface Resistivity of Concrete’s Ability to Resist Chloride Ion Penetration,” American Association of State Highway and Transportation Officials, Washington, DC, 2011.