Time Evolution of Rheology of Cement Pastes Affected by Mixture Design and Mixing Procedure

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time Evolution of Rheology of Cement Pastes Affected by Mixture Design and Mixing Procedure

Author(s): Azadeh A. Asghari, Dimitri Feys, and Geert De Schutter

Publication: Materials Journal

Volume: 115

Issue: 5

Appears on pages(s): 707-716

Keywords: cement paste; constituent elements; mixing procedure; rheology; robustness; workability loss

DOI: 10.14359/51702348

Date: 9/1/2018

Abstract:
Robustness is defined as the capacity of cement-based materials to retain fresh properties when subjected to either small variations in the constituent elements or small changes in the mixing procedure. Compared to normal concrete, self-consolidating concrete (SCC) may show less tolerance to those changes. Most robustness studies focus on initial rheological properties or workability, but concentrate less on the evolution of these properties within the first hour(s). This paper presents the results of an investigation aimed at evaluating the change of yield stress and plastic viscosity with time of cement pastes with SCC consistency, which is mainly affected by variations in the water content and the adding time of the superplasticizer. A change in water content also influences the initial rheological properties, and these differences are amplified over time. The difference due to the different adding time of the superplasticizer is, however, reduced or even reversed over time.

Related References:

1. Emborg, M., and Simonsson, P., Carlswärd, J.; and Nilsson, M., “Industrial Casting of Bridges Combining New Production Methods and Materials, Like a Robust SCC, Utilizing Lean Construction Principles,” Proceedings of the 5th International RILEM Symposium on Self-Compacting Concrete, Ghent, Belgium, 2007, pp. 485-491.

2. Bonen, D.; Deshpande, Y.; Olek, J.; Shen, L.; Struble, L.; Lange, D.; and Khayat, K., “Robustness of Self-Consolidating Concrete,” Proceedings of the 5th International RILEM Symposium on Self-Compacting Concrete, Ghent, Belgium, 2007, pp. 33-42.

3. Gettu, R.; Nawaz Shareef, S.; and Ernest, K. J. D., “Evaluation of the Robustness of SCC,” Indian Concrete Journal, V. 83, No. 6, 2009, pp. 13-19.

4. Rigueira, J. W.; García-Taengua, E.; and Serna-Ros, P., “Self-Consolidating Concrete in Continuous Production Regarding Fresh and Hardened State Properties,” ACI Materials Journal, V. 106, No. 3, May-June 2009, pp. 301-307.

5. Nunes, S.; Figueiras, H.; Oliveira, P. M.; Coutinho, J. S.; and Figueiras, J., “A Methodology to Assess Robustness of SCC Mixtures,” Cement and Concrete Research, V. 36, No. 12, 2006, pp. 2115-2122. doi: 10.1016/j.cemconres.2006.10.003

6. Billberg, P., “Increase of SCC Robustness to Varying Aggregate Moisture Content Using VMA,” Proceedings of the 2nd International Symposium on SCC, Beijing, China, 2009, pp. 473-493.

7. Naji, S.; Hwang, S.-D.; and Khayat, K. H., “Robustness of Self-­Consolidating Concrete Incorporating Different Plastic Viscosity-­Enhancing Admixtures,” ACI Materials Journal, V. 108, No. 4, July-Aug. 2011, pp. 432-438.

8. Sahmaran, M.; Yurtseven, A.; and Yaman, I. O., “Workability of Hybrid Fiber Reinforced Self-Compacting Concrete,” Building and Environment, V. 40, No. 12, 2005, pp. 1672-1677. doi: 10.1016/j.buildenv.2004.12.014

9. Ferraris, C. F.; Obla, K. H.; and Hill, R., “The Influence of Mineral Admixtures on the Rheology of Cement Paste and Concrete,” Cement and Concrete Research, V. 31, No. 2, 2001, pp. 245-255. doi: 10.1016/S0008-8846(00)00454-3

10. Han, S.; Yan, P. Y.; and Kong, X. M., “Study on the Compatibility of Cement-Superplasticizer System Based on the Amount of Free Solution,” Science China. Technological Sciences, V. 54, No. 1, 2011, pp. 183-189. doi: 10.1007/s11431-010-4174-2

11. Rubio-Hernández, F. J.; Velázquez-Navarro, J. F.; and Ordonez-Belloc, L. M., “Rheology of Concrete: A Study Case Based upon the Use of the Concrete Equivalent Mortar,” Materials and Structures, V. 46, No. 4, 2013, pp. 587-605. doi: 10.1617/s11527-012-9915-1

12. Sheinn, A. M.; Ho, D. W.; and Tam, C. T., “Rheological Model for Self-Compacting Concrete-Paste Rheology,” Proceedings of the 27th Conference on Our World in Concrete and Structures, Singapore, 2002.

13. Wallevik, J. E., “Rheological Properties of Cement Paste: Thixotropic Behavior and Structural Breakdown,” Cement and Concrete Research, V. 39, No. 1, 2009, pp. 14-29. doi: 10.1016/j.cemconres.2008.10.001

14. Tattersall, G. H., and Banfill, P. F. G., The Rheology of Fresh Concrete, Pitman, London, UK, 1983.

15. Banfill, P. F. G., “A Viscometric Study of Cement Pastes Containing Superplasticizers with a Note on Experimental Techniques,” Magazine of Concrete Research, V. 33, No. 114, 1981, pp. 37-47. doi: 10.1680/macr.1981.33.114.37

16. Douglas, R.; Gregori, A.; Sun, Z.; Bonen, D.; and Shah, S. P., “The Effect of Ingredients and Shear History on the Thixotropic Rate of Rebuilding of SCC,” Proceedings of the 2nd North American Conference and 4th International RILEM Conference on Self-Consolidating Concrete, Chicago, IL, 2005, pp. 591-596.

17. Billberg, P., “Influence of Powder Type and VMA Combination on Certain Key Fresh Properties of SCC,” Proceedings of 9th International Symposium on High Performance Concrete, Rotorua, New Zealand, 2011.

18. Li, L. G., and Kwan, A. K. H., “Concrete Mix Design Based on Water Film Thickness and Paste Film Thickness,” Cement and Concrete Composites, V. 39, No. 5, 2013, pp. 33-42. doi: 10.1016/j.cemconcomp.2013.03.021

19. Banfill, P. F. G., “A Discussion of the Papers ‘Rheological Properties of Cements Mixes’ by M. Damion and D. M. Roy,” Cement and Concrete Research, V. 9, No. 6, 1979, pp. 795-796. doi: 10.1016/0008-8846(79)90075-9

20. Flatt, R. J., “Towards a Prediction of Superplasticized Concrete Rheology,” Materials and Structures, V. 37, No. 5, 2004, pp. 289-300. doi: 10.1007/BF02481674

21. Lei, L., and Plank, J., “Synthesis, Working Mechanism and Effectiveness of a Novel Cycloaliphatic Superplasticizer for Concrete,” Cement and Concrete Research, V. 42, No. 1, 2012, pp. 118-123. doi: 10.1016/j.cemconres.2011.09.003

22. Zingg, A.; Winnefeld, F.; Holzer, L.; Pakusch, J.; Becker, S.; and Gauckler, L., “Adsorption of Polyelectrolytes and Its Influence on the Rheology, Zeta Potential, and Microstructure of Various Cement and Hydrate Phases,” Journal of Colloid and Interface Science, V. 323, No. 2, 2008, pp. 301-312. doi: 10.1016/j.jcis.2008.04.052

23. Bonen, D., and Shah, S. P., “Fresh and Hardened Properties of Self-Consolidating Concrete,” Progress in Structural Engineering Materials Journal, V. 7, No. 1, 2005, pp. 14-26. doi: 10.1002/pse.186

24. Hanehara, S., and Yamada, K., “Interaction between Cement and Chemical Admixture from the Point of Cement Hydration, Adsorption Behavior of Admixture, and Paste Rheology,” Cement and Concrete Research, V. 29, No. 8, 1999, pp. 1158-1165. doi: 10.1016/S0008-8846(99)00004-6

25. Aitcin, P. C. A.; Jolicoeur, C.; and McGregor, J. G., “Superplasticizers: How They Work and Why They Occasionally Don’t,” Concrete International, V. 16, No. 5, May 1994, pp. 45-52.

26. Roy, D. M., and Asaga, K., “Rheological Properties of Cement Mixes: III—The Effects of Mixing Procedures on Viscometric Properties of Mixes Containing Superplasticizers,” Cement and Concrete Research, V. 9, No. 6, 1979, pp. 731-739. doi: 10.1016/0008-8846(79)90068-1

27. Jones, T. E. R., and Taylor, S. A., “A Mathematical Model Relating the Flow Curve of a Cement Paste to Its Water/Cement Ratio,” Magazine of Concrete Research, V. 29, No. 101, 1977, pp. 207-212. doi: 10.1680/macr.1977.29.101.207

28. Yamada, K.; Ogawa, S.; and Hanehara, S., “Controlling of the Adsorption and Dispersing Force of Polycarboxylate-Type Superplasticizer by Sulfate Ion Concentration in Aqueous Phase,” Cement and Concrete Research, V. 31, No. 3, 2001, pp. 375-383. doi: 10.1016/S0008-8846(00)00503-2

29. Yamada, K.; Ogawa, S.; and Hanehara, S., “Working Mechanism of Poly-Beta-Naphthalene Sulfonate and Polycarboxylate Superplasticizer Types from Point of Cement Paste Characteristics,” Proceedings of the 6th CANMET/ACI International Conference on Superplasticizers and Other Chemical Admixtures in Concrete, SP-195, American Concrete Institute, Farmington Hills, MI, 2000, pp. 351-366.

30. Uchikawa, H.; Sawaki, D.; and Hanehara, S., “Influence of Kind and Added Timing of Organic Admixture on the Composition, Structure and Property of Fresh Cement Pastes,” Cement and Concrete Research, V. 25, No. 2, 1995, pp. 353-364. doi: 10.1016/0008-8846(95)00021-6

31. Kim, B. G.; Jiang, S.; Jolicoeur, C.; and Aitcin, P. C., “The Adsorption Behavior of PNS Superplasticizer and Its Relation to Fluidity of Cement Paste,” Cement and Concrete Research, V. 30, No. 6, 2000, pp. 887-893. doi: 10.1016/S0008-8846(00)00256-8

32. Jolicoeur, C.; Sharman, J.; Otis, N.; Lebel, A.; Simard, M. A.; and Page, M., “The Influence of Temperature on the Rheological Properties of Superplasticized Cement Pastes,” Proceedings of the 5th International Conference on Super-plasticizer and Other Chemical Admixtures in Concrete, Rome, Italy, 1997, pp. 379-406.

33. Simard, M. A.; Nkinamubanzi, P. C.; Jolicoeur, C.; Perraton, D.; and Aïtcin, P.-C., “Calorimetry, Rheology, and Compressive Strength of Superplasticized Cement Pastes,” Cement and Concrete Research, V. 23, No. 4, 1993, pp. 939-950. doi: 10.1016/0008-8846(93)90048-E

34. Hanna, E.; Lake, K.; Perraton, D.; and Aitcin, P. C., “Rheological Behavior of Portland Cement Paste in the Presence of a Superplasticizer,” Proceedings of the 3rd International Conference on Superplasticizers and Other Chemicals Admixtures in Concrete, SP-119, American Concrete Institute, Farmington Hills, MI, 1989, pp. 171-188.

35. Bonen, D., and Sarkar, S. L., “The Superplasticizer Adsorption Capacity of Cement Pastes Pore Solution Composition and Parameters Affecting Flow Loss,” Cement and Concrete Research, V. 25, No. 7, 1995, pp. 1423-1434. doi: 10.1016/0008-8846(95)00137-2

36. Carlsward, J.; Emborg, M.; Utsi, S.; and Oberg, P., “Effects of Constituents on the Workability and Rheology of Self-Compacting Concrete,” Proceedings of the 3rd International RILEM Symposium on Self-Compacting Concrete, O. Wallevik and I. Nielsson, eds., RILEM Publications S.A.R.L., 2003, pp. 143-153

37. Petit, J.-Y.; Khayat, K. H.; and Wirquin, E., “Coupled Effect of Time and Temperature on Variations of Yield Value of Highly Flowable Mortar,” Cement and Concrete Research, V. 36, No. 5, 2006, pp. 832-841. doi: 10.1016/j.cemconres.2005.11.001

38. Roussel, N.; Ovarlez, G.; Garrault, S.; and Brumaud, C., “The Origins of Thixotropy of Fresh Cement Pastes,” Cement and Concrete Research, V. 42, No. 1, 2012, pp. 148-157. doi: 10.1016/j.cemconres.2011.09.004

39. Kong, X.; Zhang, Y.; and Hou, S., “Study on the Rheological Properties of Portland Cement Pastes with Polycarboxylate Superplasticizers,” Rheologica Acta, V. 52, No. 7, 2013, pp. 707-718. doi: 10.1007/s00397-013-0713-7

40. Heikal, M.; Morsy, M. S.; and Aiad, I., “Effect of Treatment Temperature on the Early Hydration Characteristics of Superplasticized Silica Fume Blended Cement Pastes,” Cement and Concrete Research, V. 35, No. 4, 2005, pp. 680-687. doi: 10.1016/j.cemconres.2004.06.012

41. Jolicoeur, C., and Simard, M. A., “Chemical Admixture-Cement Interactions: Phenomenology and Physico-Chemical Concepts,” Cement and Concrete Composites, V. 20, No. 2-3, 1998, pp. 87-101. doi: 10.1016/S0958-9465(97)00062-0

42. Kreppelt, F.; Weibel, M.; Zampini, D.; and Romer, M., “Influence of Solution Chemistry on the Hydration of Polished Clinker Surfaces—A Study of Different Types of Polycarboxylic Acid-Based Admixtures,” Cement and Concrete Research, V. 32, No. 2, 2002, pp. 187-198. doi: 10.1016/S0008-8846(01)00654-8

43. Zhang, Y.; Kong, X.; Lu, Z.; Lu, Z.; and Hou, S., “Effects of the Charge Characteristics of Polycarboxylate Superplasticizers on the Adsorption and the Retardation in Cement Pastes,” Cement and Concrete Research, V. 67, 2015, pp. 184-196. doi: 10.1016/j.cemconres.2014.10.004

44. Flatt, R. J., and Bowen, P., “YODEL: A Yield Stress Model for Suspensions,” Journal of the American Ceramic Society, V. 89, No. 4, 2006, pp. 1244-1256. doi: 10.1111/j.1551-2916.2005.00888.x

45. Flatt, R. J., and Bowen, P., “Yield Stress of Multimodal Powder Suspensions: An Extension of the YODEL Yield Stress Model,” Journal of the American Ceramic Society, V. 90, No. 4, 2007, pp. 1038-1044. doi: 10.1111/j.1551-2916.2007.01595.x

46. Gołaszewski, J., and Szwabowski, J., “Influence of Superplasticizers on Rheological Behavior of Fresh Cement Mortars,” Cement and Concrete Research, V. 34, No. 2, 2004, pp. 235-248. doi: 10.1016/j.cemconres.2003.07.002

47. Struble, L., and Sun, G. K., “Viscosity of Portland Cement Paste as a Function of Concentration,” Advanced Cement Based Materials, V. 2, No. 2, 1995, pp. 62-69. doi: 10.1016/1065-7355(95)90026-8

48. Petit, J.-Y.; Wirquin, E.; and Duthoit, B., “Influence of Temperature on Yield Value of Highly Flowable Micromortars Made with Sulfonate-Based Superplasticizers,” Cement and Concrete Research, V. 35, No. 2, 2005, pp. 256-266. doi: 10.1016/j.cemconres.2004.04.025

49. Petit, J.-Y.; Khayat, K. H.; and Wirquin, E., “Coupled Effect of Time and Temperature on Variations of Plastic Viscosity of Highly Flowable Mortar,” Cement and Concrete Research, V. 39, No. 3, 2009, pp. 165-170. doi: 10.1016/j.cemconres.2008.12.007

50. Asghari, A.; Ley Hernandez, A. M.; Feys, D.; and De Schutter, G., “Which Parameters, Other Than the Water Content, Influence the Robustness of Cement Paste with SCC Consistency?” Construction and Building Materials, V. 124, 2016, pp. 95-103. doi: 10.1016/j.conbuildmat.2016.07.101

51. Reiner, M., Deformation and Flow: An Elementary Introduction to Theoretical Rheology, Lewis & Co. Limited, Great Britain, 1949.

52. Feys, D.; Wallevik, J. E.; Yahia, A.; Khayat, K. H.; and Wallevik, O. H., “Extension of the Reiner-Riwlin Equation to Determine Modified Bingham Parameters Measured in Coaxial Cylinders Rheometers,” Materials and Structures, V. 46, No. 1-2, 2013, pp. 289-311. doi: 10.1617/s11527-012-9902-6