Mitigating Alkali-Silica Reaction and Freezing and Thawing in Concrete Pavement by Silane Treatment

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mitigating Alkali-Silica Reaction and Freezing and Thawing in Concrete Pavement by Silane Treatment

Author(s): R. A. Deschenes Jr., E. R. Giannini, Thano Drimalas, B. Fournier, and W. M. Hale

Publication: Materials Journal

Volume: 115

Issue: 5

Appears on pages(s): 685-694

Keywords: alkali-silica reaction (ASR); concrete pavements; freezing and thawing (F/T); mitigation; silane

DOI: 10.14359/51702345

Date: 9/1/2018

Abstract:
Alkali-silica reaction (ASR) and freezing and thawing (F/T) cause premature deterioration and reduce the service life of concrete structures, and both are difficult to mitigate in existing concrete pavements once deterioration occurs. The objective of this research program was to evaluate the efficacy of silane surface treatments used to reduce the moisture state of concrete pavements, thereby reducing further deterioration from ASR and F/T and increasing the remaining useful life of the pavement. The pavement test section evaluated contained a borderline-reactive fine aggregate and marginal air entrainment. The efficacy of silane was evaluated by instrumenting a pavement test section with devices for monitoring strain and internal RH. Core samples were extracted before and after treatment. The core samples were evaluated using the damage rating index (DRI). Results indicate silane may reduce the rate of deterioration in the concrete pavement compared to untreated control sections.

Related References:

1. Gong, F.; Takahashi, Y.; and Maekawa, K., “Strong Coupling of Freeze-Thaw Cycles and Alkali Silica Reaction—Multi-Scale Poro-mechanical Approach to Concrete Damages,” Journal of Advanced Concrete Technology, V. 15, No. 7, 2017, pp. 346-367. doi: 10.3151/jact.15.346

2. Deschenes, R. A., “Mitigation and Evaluation of Alkali-Silica Reaction (ASR) and Freezing and Thawing in Concrete Transportation Structures,” doctoral dissertation, University of Arkansas, Fayetteville, AR, 2017, 254 pp.

3. Thomas, M. D. A.; Fournier, B.; and Folliard, K. J., “Alkali-Aggregate Reactivity (AAR) Facts Book (FHWA-HIF-13-019),” Federal Highway Administration (FHWA), U.S. Department of Transportation, Washington, DC, 212 pp.

4. Thomas, M. D. A.; Fournier, B.; Folliard, K. J.; and Resendez, B., “Alkali-Silica Reactivity Rield Identification Handbook (FHWA-HIF-12-022),” Federal Highway Administration (FHWA), U.S. Department of Transportation, Washington, DC, 2012, 80 pp.

5. Powers, T. C., “Freezing Effects in Concrete,” Durability of Concrete, SP-47, C. F. Scholer and E. Farkas, eds., American Concrete Institute, Farmington Hills, MI, 1975, pp. 1-12.

6. Tanesi, J., and Meininger, R., “Freeze-Thaw Resistance of Concrete with Marginal Air Content (FHWA-HRT-06-117),” Federal Highway Administration (FHWA), U.S. Department of Transportation, Washington, DC, 2006, pp. 1-96.

7. Powers, T. C., “A Working Hypothesis for Further Studies of Frost Resistance of Concrete,” ACI Journal Proceedings, V. 41, No. 1, Jan. 1945, pp. 245-272.

8. Bérubé, M.-A.; Chouinard, D.; Pigeon, M.; Frenette, J.; Boisvert, L.; and Rivest, M., “Effectiveness of Sealers in Counteracting Alkali-Silica Reaction in Plain and Air-Entrained Laboratory Concretes Exposed to Wetting and Drying, Freezing and Thawing, and Salt Water,” Canadian Journal of Civil Engineering, V. 29, No. 2, 2002, pp. 289-300. doi: 10.1139/l02-011

9. Sanchez, L. F. M.; Drimalas, T.; Fournier, B.; Mitchell, D.; and Bastien, J., “Comprehensive Damage Assessment in Concrete Affected by Different Internal Swelling Reaction (ISR) Mechanisms,” Cement and Concrete Research, V. 107, 2018, pp. 284-303. doi: 10.1016/j.cemconres.2018.02.017

10. Stark, D. C.; Morgan, B.; Okamoto, P.; and Diamond, S., “Eliminating or Minimizing Alkali-Silica Reactivity,” SHRP-C-343, Strategic Highway Research Program (SHRP), National Research Council, Washington, DC, 1993, 266 pp.

11. Bérubé, M.-A.; Chouinard, D.; Pigeon, M.; Frenette, J.; Rivest, M.; and Vézina, D., “Effectiveness of Sealers in Counteracting Alkali-Silica Reaction in Highway Median Barriers Exposed to Wetting and Drying, Freezing and Thawing, and Deicing Salt,” Canadian Journal of Civil Engineering, V. 29, No. 2, 2002, pp. 329-337. doi: 10.1139/l02-010

12. Thomas, M. D. A.; Folliard, K. J.; Fournier, B.; Drimalas, T.; and Rivard, P., “Study of Remedial Actions on Highway Structures Affected by ASR,” Proceedings of the 14th International Conference on Alkali-Aggregate Reaction (ICAAR), Austin, TX, 2012, 10 pp.

13. Folliard, K. J.; Thomas, M. D. A.; Fournier, B.; Resendez, Y.; Drimalas, T.; and Bentivegna, A., “Evaluation of Mitigation Measures Applied to ASR-Affected Concrete Elements: Preliminary Findings from Austin, TX Exposure Site,” Proceedings of the 14th International Conference on Alkali-Aggregate Reaction (ICAAR), Austin, TX, 2012, 10 pp.

14. Drimalas, T.; Folliard, K. J.; Thomas, M. D. A.; Fournier, B.; and Bentivegna, A., “Study of the Effectiveness of Lithium and Silane Treatments on Field Structures Affected by ASR,” Proceedings of the 14th International Conference on Alkali-Aggregate Reaction (ICAAR), Austin, TX, 2012, 10 pp.

15. Thomas, M. D. A.; Folliard, K. J.; Fournier, B.; Rivard, P.; and Drimalas, T., “Methods for Evaluating and Treating ASR-Affected Structures: Results of Field Application and Demonstration Projects (FHWA-HIF-14-0002),” Federal Highway Administration, U.S. Department of Transportation, Washington, DC, 2013, 80 pp.

16. Stark, D., “The Moisture Condition of Field Concrete Exhibiting Alkali-Silica Reactivity,” CANMET/ACI International Workshop on Alkali-Aggregate Reaction in Concrete, Halifax, NS, Canada, 1990, 19 pp.

17. Rust, C., “Role of RH in Concrete Expansion due to Alkali-Silica Reaction and Delayed Ettringite Formation: RH Thresholds, Measurement Methods, and Coatings to Mitigate Expansion,” MS thesis, University of Texas at Austin, Austin, TX, 2009, 120 pp.

18. Janssen, D., and Snyder, M., “Resistance of Concrete to Freezing and Thawing (SHRP-C-391),” Strategic Highway Research Program, National Research Council, Washington, DC, 1994, 217 pp.

19. Wehrle, E. R., “The Effects of Coatings and Sealers Used to Mitigate Alkali-Silica Reaction and/or Delayed Ettringite Formation in Hardened Concrete,” doctoral dissertation, University of Texas at Austin, Austin, TX, 2010, 166 pp.

20. Mayer, H., “The Chemistry and Properties of Silicone Resins: Network Formers (in Paints and Renders),” Pigment & Resin Technology, V. 27, No. 6, 1998, pp. 364-373. doi: 10.1108/03699429810246953

21. Fournier, B.; Bérubé, M. A.; Thomas, M. D. A.; Smaoui, N.; and Folliard, K. J., “Evaluation and Management of Concrete Structures Affected by Alkali-Silica Reaction—A Review (MTL 2004-11),” Natural Resources Canada, Ottawa, ON, Canada, 2004, 59 pp.

22. Bérubé, M. A.; Chounard, D.; Boisvert, L.; Frenetter, J.; and Pigeon, M., “Influence of Wetting-Drying and Freezing-Thawing Cycles, and Effectiveness of Sealers on ASR,” Proceedings of the 10th International Conference on Alkali-Aggregate Reaction (ICAAR), Melbourne, Australia, 1996, pp. 1056-1063.

23. Deschenes, R. A. Jr.; Murray, C. D.; and Hale, W. M., “Mitigation of Alkali-Silica Reaction and Freezing and Thawing through Surface Treatment,” ACI Materials Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 307-314. doi: 10.14359/51689493

24. Fournier, B.; Bérubé, M.-A.; Folliard, K. J.; and Thomas, M. D. A., “Report on the Diagnosis, Prognosis, and Mitigation of Alkali-Silica Reaction (ASR) in Transportation Structures (FHWA-HIF-09-004),” Federal Highway Administration, U.S. Department of Transportation, Washington, DC, 2010, 154 pp.

25. Sanchez, L.; Fournier, B.; Drimalas, B.; Bastien, J.; Mitchell, D.; and Noël, M., “Semi-quantitative Condition Assessment of Concrete Distress through the Damage Rating Index,” Proceedings of the 15th International Conference on Alkali-Aggregate Reaction (ICAAR), San Paulo, Brazil, 2016, 10 pp.

26. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; Bedoya, M. A. B.; Bastien, J.; and Duchesne, J., “Use of Damage Rating Index to Quantify Alkali-Silica Reaction Damage in Concrete: Fine versus Coarse Aggregate,” ACI Materials Journal, V. 113, No. 4, July-Aug. 2016, pp. 395-407. doi: 10.14359/51688983

27. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; Mitchell, D.; and Bastien, J., “Overall Assessment of Alkali-Aggregate Reaction (AAR) in Concretes Presenting Different Strengths and Incorporating a Wide Range of Reactive Aggregate Types and Natures,” Cement and Concrete Research, V. 93, 2017, pp. 17-31. doi: 10.1016/j.cemconres.2016.12.001

28. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; and Duchesne, J., “Reliable Quantification of AAR Damage through Assessment of the Damage Rating Index (DRI),” Cement and Concrete Research, V. 67, 2015, pp. 74-92. doi: 10.1016/j.cemconres.2014.08.002

29. Rivard, P.; Founrier, B.; and Ballivy, G., “The Damage Rating Index Method for ASR Affected Concrete—A Critical Review of Petrographic Features of Deterioration and Evaluation Criteria,” Cement, Concrete and Aggregates, V. 24, No. 2, 2002, pp. 1-11.

30. Grattan-Bellew, P. E., and Mitchell, L. D., “Quantitative Petrographic Analysis of Concrete—The Damage Rating Index (DRI) Method, A Review,” Proceedings of the Marc-André Bérubé Symposium on AAR in Concrete: CANMET/ACI Advances in Concrete Technology Seminar, Montréal, QC, Canada, pp. 321-334.

31. Dunbar, P. A., and Grattan-Bellew, P. E., “Results of Damage Rating Evaluation of Condition of Concrete from a Number of Structures Affected by ASR,” CANMET/ACI International Workshop on Alkali-Aggregate Reactions in Concrete, Dartmouth, NS, Canada, pp. 257-266.

32. Shrimer, F., “Application and Use of Damage Rating Index in Assessment of AAR-Affected Concrete—Selected Case Studies,” Proceedings of the 11th International Conference on Alkali Aggregate Reaction (ICAAR), Quebec, QC, Canada, 2000, pp. 899-907.

33. Villeneuve, V.; Fournier, B.; and Duchesne, J., “Determination of the Damage in Concrete Affected by ASR—The Damage Rating Index (DRI),” Proceedings of the 14th International Conference on Alkali-Aggregate Reaction (ICAAR), Austin, TX, 2012, 10 pp.

34. Deschenes, R. Jr., and Hale, W. M., “Alkali-Silica Reaction in Concrete with Previously Inert Aggregates,” Journal of Performance of Constructed Facilities, V. 31, No. 2, Apr. 2016, 10 pp.

35. Construction Technology Laboratories Group, “Petrographic Examination of Concrete Specimens from I-540 Roadway and Barrier Wall (Project No. 157501),” CTLGroup, Skokie, IL, 2012, 17 pp.

36. Tremblay, S.; Fournier, B.; Thomas, M. D. A.; and Folliard, K. J., “The Lomas Boulevard Road Test Site, Albuquerque, NM. Case Study on the Use of Preventive Measures against ASR in New Concrete,” Proceedings of the 14th International Conference on Alkali-Aggregate Reaction (ICAAR),” Austin, TX, 2012, 10 pp.

37. ASTM C1260-05, “Standard Test Method for Potential Alkali Reactivity of Aggregates (Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2005, 5 pp.

38. ASTM C1293-08b, “Standard Test Method for Determination of Length Change of Concrete due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2008, 10 pp.

39. Reed, R.; Deschenes Jr., R. A.; and Hale, W. M., “Measuring Relative Humidity in Concrete Pavements as a Method to Assess ASR Mitigation Measures,” Proceedings of the 15th International Conference on Alkali-Aggregate Reaction (ICAAR), San Paulo, Brazil, 2016, 9 pp.

40. Waidner, M., “Identifying Damage, Predicting Expansion, and Determining the Effectiveness of Sealers on Concrete Affected by Alkali-Silica Reaction and Freeze-Thaw,” master’s thesis, University of Arkansas, Fayetteville, AR, 2015, 88 pp.

41. Sanchez, L. F. M.; Fournier, B.; Jolin, M.; Mitchell, D.; and Bastien, J., “Overall Assessment of Alkali-Aggregate Reaction (AAR) in Concretes Presenting Different Strengths and Incorporating a Wide Range of Reactive Aggregate Types and Natures,” Cement and Concrete Research, V. 93, 2017, pp. 17-31. doi: 10.1016/j.cemconres.2016.12.001


ALSO AVAILABLE IN:

Electronic Materials Journal