Exterior Ultra-High-Performance Concrete Thin Wall Cladding Panels & Building Code Compliance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Exterior Ultra-High-Performance Concrete Thin Wall Cladding Panels & Building Code Compliance

Author(s): Mahmut Ekenel

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 4/4/2018

Abstract:
Ultra-high-performance concrete (UHPC) is seen as an influential material innovation in the construction industry in the twenty first century. Many research groups overseas as well as in the United States have studied the material and structural behavior in the last two decades. One of the most critical challenges is finding innovative approaches in material design, quality control, and structural performance to strengthen the broad application of this material. UHPC is a preferable construction material of the twenty-first century due to its excellent strength, durability, ductility, and energy dissipation capacity. The session will invite national and international research groups, material suppliers, and contractors to share their knowledge in innovations for broad application. This session fits naturally into the theme “Driving Concrete Technology.”