Experimental Investigation of PCC Incorporating RAP

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Investigation of PCC Incorporating RAP

Author(s): Sawssen El Euch Ben Said, Saloua El Euch Khay, Amara Loulizi

Publication: IJCSM

Volume: 12

Issue:

Appears on pages(s):

Keywords: portland cement, recycled asphalt pavement, heat of hydration, semi-adiabatic, shrinkage, rigid pavements, sustainability.

DOI: 10.1186/s40069-018-0227-x

Date: 1/31/2018

Abstract:
Rehabilitation and repair of flexible pavements produce huge amounts of reclaimed asphalt pavement (RAP) material. Using RAP in the formulation of portland cement concrete (PCC) is a technique that is part of a sustainable development approach since it reduces on the consumption of new aggregates and reuses a material that is considered as waste. This paper describes the semi-adiabatic calorimetry test performed on a concrete mix incorporating RAP material as aggregate. Results showed that the cement hydration process is not affected by the presence of asphalt coated on the surface of RAP material. Classical tests (compressive strength, flexural and indirect-tensile strengths, elastic modulus, and free-shrinkage) were also performed on PCC mixes incorporating different percentages of RAP. It was found that as the percentage of RAP increases, the PCC mechanical properties decrease. This is mainly attributed to the presence of voids in the transition zone between the asphalt-coated aggregates and the hydrated cement paste as confirmed by scanning-electron microscope images. Unrestrained shrinkage testing showed statistically insignificant change in shrinkage strain with RAP content. The strength and shrinkage results lead to conclude that as much as 40% of RAP could be incorporated into the formulation of PCC and achieve properties that are acceptable for the construction of rigid pavements.