Exploring the Potential of a New Type of CFRP Laminate and Technique for the Strengthening of RC Structures

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Exploring the Potential of a New Type of CFRP Laminate and Technique for the Strengthening of RC Structures

Author(s): Joaquim A. O. Barros, Mohammadali Rezazadeh, and Honey Ramezansefat

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/16/2018

Abstract:
This session targets the application of advanced analytical techniques for the analysis and design of fiber-reinforced polymer (FRP) strengthened concrete structures, with an emphasis on structure and member behavior, as well as debonding and anchorage devices. It will be suitable to designers of FRP strengthening measures as well as researchers and manufacturers.