Title: Collapse Assessment of RC Structures

Author(s): Riadh Al-Mahaidi, Javad Hashemi, Yassamin Al-Ogaidi, Robin Kalfat, and John Wilson

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/16/2018

Abstract:
This session targets the application of advanced analytical techniques for the analysis and design of fiber-reinforced polymer (FRP) strengthened concrete structures, with an emphasis on structure and member behavior, as well as debonding and anchorage devices. It will be suitable to designers of FRP strengthening measures as well as researchers and manufacturers.