Effects of Reduced Paste Content and Base Restraint on Young Concrete Pavement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Reduced Paste Content and Base Restraint on Young Concrete Pavement

Author(s): D. G. Mapa, A. Markandeya, A. Sedaghat, N. Shanahan, H. DeFord, K. A. Riding, and A. Zayed

Publication: Materials Journal

Volume: 115

Issue: 5

Appears on pages(s): 663-673

Keywords: bond breaker; concrete pavement repair; jointed plain concrete pavement; paste content reduction; stressmeter

DOI: 10.14359/51702241

Date: 9/1/2018

Abstract:
Jointed plain concrete pavement (JPCP) replacement slabs can experience early-age cracking from early-age volume change. These slabs are often made of high-early-strength (HES) concrete characterized by high cement content and low water-cement ratio (w/c), which can result in large temperature rise and high levels of autogenous shrinkage, and ultimately an elevated cracking potential. This study investigated the effects of reduced paste content and base restraint minimization on reducing concrete early-age cracking potential. The effect of each of these measures was evaluated in place by measuring the stress and temperature development in concrete test slabs instrumented with concrete stressmeters and thermocouples. Calorimetry studies and mechanical properties testing were used with modeling software to assess field trends. The findings indicated that it is possible to achieve higher strengths and lower stresses with low-paste mixtures. Changes in concrete stress during the first 24 hours after placement, due to moisture loss to the base, were seen in slabs with polyethylene sheet or geotextile fabric underneath the slab.

Related References:

1. Zayed, A.; Riding, K.; Ferraro, C. C.; Bien-aime, A.; Shanahan, N.; Buidens, D.; Meagher, T.; Tran, V.; Henika, J. D.; Paris, J. M.; Tibbetts, C. M.; and Watts, B. E., “Final Report Long-Life Slab Replacement Concrete FDOT Contract Number : BDV25-977-01,” University of South Florida, Tampa, FL, 2015, 306 pp.

2. Florida DOT, “Standard Specifications for Road and Bridge Construction,” Tallahassee, FL, 2016, 1206 pp.

3. VanDam, T. J.; Peterson, K. R.; Sutter, L. L.; Panguluri, A.; and Sytsma, J., “Guidelines for Early-Opening to Traffic Portland Cement Concrete for Pavement Rehabilitation, NCHRP Report 540,” National Cooperative Highway Research Program, Transportation Research Board, Washington, DC, 2005, 37 pp.

4. Taylor, P. C.; Kosmatka, S. H.; and Voigt, G. F., “Integrated Materials and Construction Practices for Concrete Pavement: A State-of-the-Practice Manual,” National Concrete Pavement Technology Center, Iowa State University, Ames, IA, 2006, 346 pp.

5. Meagher, T.; Shanahan, N.; Buidens, D.; Riding, K. A.; and Zayed, A., “Effects of Chloride and Chloride-Free Accelerators Combined with Typical Admixtures on the Early-Age Cracking Risk of Concrete Repair Slabs,” Construction and Building Materials, V. 94, 2015, pp. 270-279. doi: 10.1016/j.conbuildmat.2015.07.003

6. Shanahan, N.; Bien-Aime, A.; Buidens, D.; Meagher, T.; Sedaghat, A.; Riding, K.; and Zayed, A., “Combined Effect of Water Reducer – Retarder and Variable Chloride-Based Accelerator Dosage on Rapid Repair Concrete Mixtures for Jointed Plain Concrete Pavement,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 7, 2016, pp. 1-10.

7. Yurdakul, E., “Proportioning for Performance-Based Concrete Pavement Mixtures,” PhD dissertation, Iowa State University, Ames, IA, 2010, 227 pp.

8. Koehler, E. P., and Fowler, D. W., “ICAR Mixture Proportioning Procedure for Self-Consolidating Concrete: 108-1,” International Center for Aggregates Research, University of Texas at Austin, Austin, TX, 24 pp.

9. Wang, X.; Taylor, P.; Wang, K.; and Morcous, G., “Effects of Paste-to-Voids Volume Ratio on Performance of Self-Consolidating Concrete Mixtures,” Magazine of Concrete Research, V. 67, No. 14, 2014, pp. 771-785. doi: 10.1680/macr.14.00313

10. Obla, K.; Lobo, C.; Hong, R.; and Kim, H., Optimizing Concrete Mixtures for Performance and Sustainability, National Ready Mixed Concrete Association, Silver Spring, MD, 2015, 59 pp.

11. Moini, M.; Flores-Vivian, I.; Amirjanov, A.; and Sobolev, K., “The Optimization of Aggregate Blends for Sustainable Low Cement Concrete,” Construction and Building Materials, V. 93, 2015, pp. 627-634. doi: 10.1016/j.conbuildmat.2015.06.019

12. Fennis, S. A. A. M., and Walraven, J. C., “Using Particle Packing Technology for Sustainable Concrete Mixture Design,” Heron, V. 57, No. 2, 2012, pp. 73-101.

13. Fuller, W. B., and Thompson, S. E., “The Laws Of Proportioning Concrete,” Asian Journal of Civil Engineering, V. 59, 1907, pp. 67-143.

14. Shilstone, J. M., and Shilstone, J. M., “Performance-Based Concrete Mixtures and Specifications for Today,” Concrete International, V. 24, No. 2, Feb. 2002, pp. 80-83.

15. Goltermann, P.; Johansen, V.; and Palbol, L., “Packing of Aggregates: An Alternative Tool to Determine the Optimal Aggregate Mix,” ACI Materials Journal, V. 94, No. 5, Sept.-Oct. 1997, pp. 435-443.

16. Anderson, P., and Johansen, V., “A Guide to Determining the Optimal Gradation of Concrete Aggregates,” Strategic Highway Research Program, Washington, DC, 1993, 201 pp.

17. Yurdakul, E.; Taylor, P. C.; Ceylan, H.; and Bektas, F., “Effect of Paste-to-Voids Volume Ratio on the Performance of Concrete Mixtures,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 12, 2013, pp. 1840-1851. doi: 10.1061/(ASCE)MT.1943-5533.0000728

18. Knoppik-Wróbel, A., and Klemczak, B., “Degree of Restraint Concept in Analysis of Early-Age Stresses in Concrete Walls,” Engineering Structures, V. 102, Nov. 2015, pp. 369-386. doi: 10.1016/j.engstruct.2015.08.025

19. Rasmussen, R. O., and Rozycki, D. K., “Characterization and Modeling of Axial Slab-Support Restraint,” Transportation Research Record: Journal of the Transportation Research Board, V. 1778, 2001, pp. 26-32. doi: 10.3141/1778-04

20. Wesevich, J. W.; Mccullough, B. F.; and Burns, N. H., “Stabilized Subbase Friction Study for Concrete Pavements,” Center for Transportation Research, University of Texas at Austin, Austin, TX, 1987, 197 pp.

21. Li, S.; Tian, B.; Niu, K.; Sun, Z.; and Zhou, W., “Characteristics of Base Friction for Concrete Pavement Structure in China,” Transportation Research Record: Journal of the Transportation Research Board, V. 2367, No. 1, 2013, pp. 107-112. doi: 10.3141/2367-11

22. Pittman, D. W., and McCullough, B., “Development of a Roller-Compacted Concrete Pavement Crack and Joint,” Transportation Research Record: Journal of the Transportation Research Board, V. 1568, 1997, pp. 52-64. doi: 10.3141/1568-07

23. Zhang, T.; Yao, J.; Yuan, J.; and Yao, D., “Experimental Study and Mechanism Analysis on an Emulsion Wax Curing Agent Used in a Cement-Stabilized Granular Base,” Proceedings of the Fourth Geo-China International Conference, Shandong, China, 2016, pp. 109-117.

24. Chia, W. S.; Mccullough, B. F.; and Burns, N. H., “Field Evaluation of Subbase Friction Characteristics,” Center for Transportation Research, University of Texas at Austin, Austin, TX, 1986, 90 pp.

25. Maitra, S. R.; Reddy, K. S.; and Ramachandra, L. S., “Experimental Evaluation of Interface Friction and Study of Its Influence on Concrete Pavement Response,” Journal of Transportation Engineering, ASCE, V. 135, No. 8, 2009, pp. 563-572. doi: 10.1061/(ASCE)0733-947X(2009)135:8(563)

26. Zhang, J., and Li, V. C., “Influence of Supporting Base Characteristics on Shrinkage-Induced Stresses in Concrete Pavements,” Journal of Transportation Engineering, ASCE, V. 127, No. 6, 2001, pp. 455-462. doi: 10.1061/(ASCE)0733-947X(2001)127:6(455)

27. Federal Highway Administration, “I-29 Reconstruction Evaluation of Geotextile Interlayer,” Federal Highway Administration, Washington, DC, 2007, 18 pp.

28. Suh, Y. C.; Lee, S. W.; and Kang, M. S., “Evaluation of Subbase Friction for Typical Korean Concrete Pavement,” Transportation Research Record: Journal of the Transportation Research Board, V. 1809, 2002, pp. 66-73.

29. Hall, K.; Danwood, D.; Vanikar, S.; Tally, R.; Cackler, T.; Angel, C.; Peter, D.; James, D.; Geary, G.; Gisi, A.; Hanna, A.; Kosmatka, S.; Rasmussen, R. O.; Tayabji, S.; and Voigt, G., “Longilife Concrete Pavements in Europe and Canada,” American Trade Initiatives, Alexandria, VA, 2007, 84 pp.

30. ASTM C33/C33M-16, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2016, 11 pp.

31. ASTM C29/C29M-16, “Standard Test Method for Bulk Density (‘Unit Weight’) and Voids in Aggregate,” ASTM International, West Conshohocken, PA, 2016, 5 pp.

32. ASTM C127-15, “Standard Test Method for Relative Density (Specific Gravity) and Absorption of Coarse Aggregate,” ASTM International, West Conshohocken, PA, 2015, 5 pp.

33. ASTM C128-15, “Standard Test Method for Relative Density (Specific Gravity) and Absorption of Fine Aggregate,” ASTM International, West Conshohocken, PA, 2015, 6 pp.

34. ASTM C494/C494M-16, “Standard Specification for Chemical Admixtures for Concrete,” ASTM International, West Conshohocken, PA, 2016, 10 pp.

35. ASTM C260/C260M-10a, “Standard Specification for Air-Entraining Admixtures for Concrete,” ASTM International, West Conshohocken, PA, 2016, 4 pp.

36. Poole, J. L., “Modeling Temperature Sensitivity and Heat Evolution of Concrete,” PhD dissertation, University of Texas at Austin, Austin, TX, 2007, 608 pp.

37. Reinert, S. K., “Optimizing Portland Cement Concrete Mix Design to Environmental and Construction Variables with the Aid of Computer Design Software,” master’s thesis, Iowa State University, Ames, IA, 2007, 112 pp.

38. Taylor, P.; Yurdakul, E.; and Brink, M., “Performance-Based Proportioning: An Innovative Approach and Tool for Concrete Mixtures,” Concrete International, V. 37, No. 8, Aug. 2015, pp. 41-46.

39. Yurdakul, E., “Optimizing Concrete Mixtures with Minimum Cement Content for Performance and Sustainability,” master’s thesis, Iowa State University, Ames, IA, 2010, 120 pp.

40. ASTM C39/39M-15a, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015, 8 pp.

41. ASTM C496/C496M-11, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2011, 5 pp.

42. ASTM C469/C469M-14, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014, 5 pp.

43. ASTM C1702-14, “Standard Test Method for Measurement of Heat of Hydration of Hydraulic Cementitious Materials Using Isothermal Conduction Calorimetry,” ASTM International, West Conshohocken, PA, 2014, 8 pp.

44. Poole, J. L.; Riding, K. A.; Folliard, K. J.; Juenger, M. C. G.; and Schindler, A. K., “Methods for Calculating Activation Energy for Portland Cement,” ACI Materials Journal, V. 104, No. 1, Jan.-Feb. 2007, pp. 303-311.

45. RILEM Technical Committee 119-TCE., “Adiabatic and Semi-Adiabatic Calorimetry to Determine the Temperature Increase in Concrete Due to Hydration Heat of the Cement,” Materials and Structures, V. 30, No. 8, 1998, pp. 451-464.

46. ASTM C192/192M 2007, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2010, 8 pp.

47. Transtec Group, “HIPERPAV III (v3.20.0006),” 2009, www.hiperpav.com. (last accessed July 16, 2018)

48. Ruiz, J. M.; Kim, P. J.; Schindler, A. K.; and Rasmussen, R. O., “Validation of HIPERPAV for Prediction of Early-Age Jointed Concrete Pavement,” Transportation Research Record: Journal of the Transportation Research Board, V. 1778, 2001, pp. 17-25. doi: 10.3141/1778-03

49. Otto Rasmussen, R.; Mauricio Ruiz, J.; Rozycki, D.; and Frank McCullough, B., “Constructing High-Performance Concrete Pavements with FHWA HIPERPAV Systems Analysis Software,” Transportation Research Record: Journal of the Transportation Research Board, V. 1813, 2002, pp. 11-20. doi: 10.3141/1813-02

50. Xu, Q.; Ruiz, J. M.; Chang, G. K.; Rasmussen, R. O.; and Rozycki, D. K., “Moisture Transport Model for Enhancing FHWA HIPERPAV Predictions,” Transportation Research Record: Journal of the Transportation Research Board, V. 2113, No. 1, 2009, pp. 1-12. doi: 10.3141/2113-01

51. McCullough, B. F., and Rasmussen, R. O., “Fast Track Paving: Concrete Temperature Control and Traffic Opening Criteria for Bonded Concrete Overlays Volume I -Final Report,” Transtec Inc., Austin, TX, 1998, 204 pp.

52. McCullough, B. F., and Rasmussen, R. O., “Fast Track Paving: Concrete Temperature Control and Traffic Opening Criteria for Bonded Concrete Overlays Volume II -HIPERPAV User’s Manual,” Transtec Inc., Austin, TX, 1999, 77 pp.

53. Transtec Inc., “HIPERPAV Technical Memorandum, TM30-A: Sensitivity and Behavior Analysis of HIPERPAV for Group 1, 2, and 3 Input Parameters,” Austin, TX, 1999, 6 pp.

54. Transtec Inc., “HIPERPAV Technical Memorandum, TM30-B: Sensitivity and Behavior Analysis of HIPERPAV for Group 4 and 5 Input Parameters,” Austin, TX, 1999, 5 pp.

55. Transtec Inc., “HIPERPAV Technical Memorandum, TM30-C: Sensitivity and Behavior Analysis of HIPERPAV for Group 6 and 7 Input Parameters,” Austin, TX, 1999, 5 pp.

56. ASTM C1074-11, “Standard Practice for Estimating Concrete Strength by the Maturity Method,” ASTM International, West Conshohocken, PA, 2011, 10 pp.

57. Concrete Durability Center, “ConcreteWorks (v3.1.0),” 2007, https://www.txdot.gov/inside-txdot/division/information-technology/engineering-software.external.html. (last accessed July 16, 2018)

58. Riding, K. A., “Early Age Concrete Thermal Stress Measurement and Modeling,” PhD dissertation, University of Texas at Austin, Austin, TX, 2007, 611 pp.

59. Zingg, A.; Winnefeld, F.; Holzer, L.; Pakusch, J.; Becker, S.; Figi, R.; and Gauckler, L., “Interaction of Polycarboxylate-Based Superplasticizer with Cements Containing Different C3A Amounts,” Cement and Concrete Composites, V. 31, No. 3, 2009, pp. 153-162. doi: 10.1016/j.cemconcomp.2009.01.005

60. Winnefeld, F.; Becker, S.; Pakusch, J.; and Götz, T., “Effects of the Molecular Architecture of Comb-Shaped Superplasticizers on Their Performance in Cementitious Systems,” Cement and Concrete Composites, V. 29, No. 4, 2007, pp. 251-262. doi: 10.1016/j.cemconcomp.2006.12.006

61. Lothenbach, B.; Winnefeld, F.; and Figi, R., “The Influence of Superplasticizers on the Hydration of Portland Cement,” Proceedings of the 12th ICCC, 2007, pp. 1-12.

62. Xu, Q.; Hu, J.; Ruiz, J. M.; Wang, K.; and Ge, Z., “Isothermal Calorimetry Tests and Modeling of Cement Hydration Parameters,” Thermochimica Acta, V. 499, No. 1-2, 2010, pp. 91-99. doi: 10.1016/j.tca.2009.11.007

63. ACI Committee 231, “Early-Age Cracking: Causes, Measurement, and Mitigation (ACI 231R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 50 pp.

64. Lee, E. B.; Lamour, V.; Pae, J. H.; and Harvey, J., “Analysis of Sensitivity of Plain Jointed Concrete Pavement in California to Early-Age Cracking Using HIPERPAV,” University of California, Pavement Research Center, Davis, CA, 2003, 72 pp.