Shear Strengthening of Concrete Girders Using Carbon Fiber-Reinforced Polymer Sheets and Anchors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strengthening of Concrete Girders Using Carbon Fiber-Reinforced Polymer Sheets and Anchors

Author(s): Jose E. Garcia, C. Neil Satrom, James O. Jirsa, and Wassim M. Ghannoum

Publication: Structural Journal

Volume: 115

Issue: 4

Appears on pages(s): 1165-1173

Keywords: bidirectional carbon fiber-reinforced polymer (CFRP) layout; CFRP anchor; CFRP strip; I-girder; reentrant corners; shear strengthening

DOI: 10.14359/51702234

Date: 7/1/2018

Abstract:
Four 1.4 m (54 in.) prestressed concrete I-girders were tested to evaluate the feasibility of using carbon fiber-reinforced polymer (CFRP) sheets and anchors to increase the shear capacity of large prestressed concrete members. One specimen was a control test with no strengthening. CFRP sheets were applied in the vertical direction for one test and in the vertical and horizontal directions for two tests. CFRP anchors were used to anchor the CFRP strips and to provide for transfer of stresses from the strip to the concrete when the CFRP strip debonded. The unidirectional application of CFRP resulted in a higher shear cracking load but no significant increase in shear capacity. The addition of horizontal CFRP strips led to almost a 40% increase in shear strength. The addition of CFRP also resulted in increased shear deformation capacity before failure. An important aspect of the study was the use of anchors at reentrant corners, such as those at the top and bottom of the web of an I-girder, to allow the development of the CFRP strip capacity on a non-rectangular section.

Related References:

1. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 76 pp.

2. Kim, Y.; Quinn, K.; Satrom, C. N.; Garcia, J.; Sun, W.; Ghannoum, W. M.; and Jirsa, J. O., “Shear Strengthening of Reinforced and Prestressed Concrete Beams Using Carbon Fiber Reinforced Polymer (CFRP) Sheets and Anchors,” Report 0-6306-1, Center for Transportation Research at The University of Texas at Austin, Austin, TX, 2012, pp. 226-229.

3. Triantafillou, T. C., “Shear Strengthening of Reinforced Concrete Beams Using Epoxy-Bonded FRP Composites,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 107-115.

4. Kim, I.; Jirsa, J. O.; and Bayrak, O., “Anchorage of Carbon Fiber-Reinforced Polymer on Side Faces of Reinforced Concrete Beams to Provide Continuity,” ACI Structural Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 1089-1098.

5. Kim, C.; Ghannoum, W. M.; and Jirsa, J. O., “Behavior of Reinforced Concrete Panels Strengthened with Carbon Fiber-Reinforced Polymers,” ACI Structural Journal, V. 113, No. 6, Sept.-Oct. 2016, pp. 1077-1084.

6. AASHTO, “LRFD Bridge Design Specifications,” American Association of Highway Transportation Officials, Washintgon, DC, 2010, pp. 5-1 to 5-265.


ALSO AVAILABLE IN: