Proposed Development Length Equation for Plain Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Proposed Development Length Equation for Plain Bars

Author(s): Lisa R. Feldman, Umesh Poudyal, and John Cairns

Publication: Structural Journal

Volume: 115

Issue: 6

Appears on pages(s): 1615-1623

Keywords: bar shape; bar size; casting position; development length; historical structures; lap splice; plain reinforcement; structural evaluation; structural safety

DOI: 10.14359/51702230

Date: 11/1/2018

Abstract:
ACI 562-16 permits development and splice lengths of plain reinforcing bars to be assessed using code provisions that were in effect at the time of construction. However, previous research has shown that margins of safety provided by these provisions varied markedly between successive code editions and were unsafe for certain scenarios. A reliability-based equation, calibrated for safety in accordance with U.S. practice, is therefore developed from a test database of 29 viable splice specimens and 268 beam-end specimens. The subsequent comparison of results provided for plain bars using the proposed equation and those included in ACI 318-14 for deformed bars suggest that the historical rule-of-thumb that bottom-cast plain round bars require twice the development length of deformed bars is likely slightly conservative, while the considerable top-cast effect for plain bars results in their development length being almost three times that required for deformed bars.

Related References:

1. ACI Committee 318, “Building Code Requirements for Reinforced Concrete (ACI 318-63),” American Concrete Institute, Farmington Hills, MI, 1963, 148 pp.

2. ACI Committee 562, “Code Requirements for Evaluation, Repair and Rehabilitation of Concrete Buildings (ACI 562-16) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2016, 88 pp.

3. Feldman, L. R., and Cairns, J., “Assessing Historical Provisions for Bond of Plain Bars,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 463-473. doi: 10.14359/51689163

4. Abrams, D. A., “Tests of Bond between Concrete and Steel,” University of Illinois Bulletin No. 71, University of Illinois at Urbana-Champaign, Urbana, IL, 1913, 240 pp.

5. Menzel, C. A., and Woods, W. M., “An Investigation of Bond, Anchorage and Related Factors in Reinforced Concrete Beams,” Research and Development Laboratories of the Portland Cement Association Research Department Bulletin 42, Portland Cement Association, Chicago, IL, 1952, 65 pp.

6. Joint ACI-ASCE Committee 408, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03) (Reapproved 2012),” American Concrete Institute, Farmington Hills, MI, 2012, 62 pp.

7. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

8. Hassan, M. N., and Feldman, L. R., “Behavior of Lap-Spliced Plain Steel Bars,” ACI Structural Journal, V. 109, No. 2, Mar.-Apr. 2012, pp. 235-244.

9. Sekulovic MacLean, M., and Feldman, L. R., “Effects of Casting Position and Bar Shape on Bond of Plain Bars,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 323-330.

10. Poudyal, U., and Feldman, L. R., “Towards Development Length Criteria for Plain Reinforcing Bars in Tension,” 2017 Annual Conference of the Canadian Society for Civil Engineering, Vancouver, BC, Canada, 2017, 10 pp.

11. Chana, P. S., “A Test Method to Establish Realistic Bond Stresses,” Magazine of Concrete Research, V. 42, No. 151, 1990, pp. 83-90. doi: 10.1680/macr.1990.42.151.83

12. Metzinger, H., “Bond of Plain Round Bars,” internal report, Heriot-Watt University, Edinburgh, UK, 2002.

13. Cairns, J.; Du, Y.; and Law, D. W., “Residual Bond Strength of Corroded Plain Round Bars,” Magazine of Concrete Research, V. 58, No. 4, 2006, pp. 221-231. doi: 10.1680/macr.2006.58.4.221

14. Snowdon, L. C., “Classifying Reinforcing Bars for Bond Strength,” Building Research Establishment, Garston, England, 1970, 37 pp.

15. Baldwin, M. I., and Clark, L. A., “The Assessment of Reinforcing Bars with Inadequate Anchorage,” Magazine of Concrete Research, V. 47, No. 171, 1995, pp. 95-102. doi: 10.1680/macr.1995.47.171.95

16. Kankam, C. K., “Relationship of Bond Stress, and Slip in Reinforced Concrete,” Journal of Structural Engineering, ASCE, V. 123, No. 1, 1997, pp. 79-85. doi: 10.1061/(ASCE)0733-9445(1997)123:1(79)

17. Bamonte, P.; Coronelli, D.; and Gambarova, P., “Smooth Anchored Bars in NSC & HPC: A Study on Size Effect,” Journal of Advanced Concrete Technology, V. 1, No. 1, 2003, pp. 42-53. doi: 10.3151/jact.1.42

18. Vranas, P., “Effect of Test Geometry and Test Sequence on Bond of Reinforcement Bars,” Research Project CEM4A4, The University of Birmingham, Birmingham, UK, 119 pp.

19. Darwin, D., “Tension Development Length and Lap Splice Design for Reinforced Concrete Members,” Progress in Structural Engineering and Materials, V. 7, No. 4, 2005, pp. 210-225. doi: 10.1002/pse.206

20. Feldman, L. R., and Bartlett, F. M., “Bond Strength Variability in Pullout Specimens with Plain Reinforcement,” ACI Structural Journal, V. 102, No. 6, Nov.-Dec. 2005, pp. 860-867.

21. Zuo, J., and Darwin, D., “Splice Strength of Conventional and High Relative Rib Area Bars in Normal and High-Strength Concrete,” ACI Structural Journal, V. 97, No. 4, July-Aug. 2000, pp. 630-641.

22. Darwin, D., personal correspondence, March 19, 2017.

23. Bischoff, P. H., and MacLaggan, D. A., “Bond and Tension Stiffening in Concrete Tension Members with Plain Reinforcement,” 2006 Annual Conference of the Canadian Society for Civil Engineering, Calgary, AB, Canada, 2006, 10 pp.

24. Bischoff, P. H., and Johnson, R. D., “Effect of Bond and Cracking on Serviceability Related Behaviour of Concrete Beams Reinforced with Plain (Undeformed) Reinforcing Bars,” 2008 Annual Conference of the Canadian Society for Civil Engineering, Québec, QC, Canada, 2008, 8 pp.

25. Orangun, C. O.; Jirsa, J. O.; and Breen, J. E., “The Strength of Anchor Bars: A Reevaluation of Test Data on Development Length and Splices,” Research Report 154-3F, Center for Highway Research, The University of Texas at Austin, Austin, TX, 1975, 78 pp.

26. Feldman, L. R., and Bartlett, F. M., “Bond in Flexural Members with Plain Steel Reinforcement,” ACI Structural Journal, V. 105, No. 5, Sept.-Oct. 2008, pp. 552-560.

27. Orangun, C. O.; Jirsa, J. O.; and Breen, J. E., “A Reevaluation of Test Data on Development Length and Splices,” ACI Journal Proceedings, V. 74, No. 3, Mar. 1977, pp. 114-122.


ALSO AVAILABLE IN:

Electronic Structural Journal