Out-of-Plane Flexural Behavior of Reinforced Masonry Walls Strengthened with Near-Surface-Mounted Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Out-of-Plane Flexural Behavior of Reinforced Masonry Walls Strengthened with Near-Surface-Mounted Fiber-Reinforced Polymer

Author(s): Zuhair Al-Jaberi, John J. Myers, and Mohamed A. ElGawady

Publication: Structural Journal

Volume: 115

Issue: 4

Appears on pages(s): 997-1010

Keywords: cyclic load; fiber-reinforced polymer; masonry walls; nearsurface- mounted; out-of-plane; strengthening

DOI: 10.14359/51702227

Date: 7/1/2018

Abstract:
Eighteen reinforced masonry walls were built as a part of this study. These reinforced walls were strengthened with carbon fiber reinforced polymer (FRP) bars and strips and glass FRP bars using a near-surface-mounted (NSM) technique; different mild steel reinforcement ratios (ρ) were used. These simply supported walls were tested under an out-of-plane cyclic load that was applied along two line loads. Various parameters were investigated, including those related to FRP (type and amount), bond pattern (stack and running), mortar pattern (face shell bedding and fully bedding), embedding material (epoxy and cementitious paste), amount of internal steel reinforcement, existence of compression FRP bars, and groove size. The ultimate load, deflection at ultimate load, and mode of failure were investigated in this study. The test results indicated a significant increase in stiffness and flexural capacity of out-of-plane reinforced walls strengthened with FRP compared to the unstrengthened reinforced walls. Different modes of failure occurred in the strengthened reinforced walls, including flexure-shear failure through the concrete block, as well as debonding of FRP reinforcement from the masonry substrate. Furthermore, a simple analytical model for computing the moment capacity of strengthened reinforced masonry walls is proposed and compared with the experimental results.

Related References:

ACI Committee 440, 2006, “Guide for the Design and Construction of Concrete Reinforced with FRP Bars (ACI 440.1R-06),” American Concrete Institute, Farmington Hills, MI, 44 pp.

ACI Committee 440, 2008, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 76 pp.

ACI Committee 440, 2010, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Masonry Structures (ACI 440.7R-10),” American Concrete Institute, Farmington Hills, MI, 46 pp.

Al-Jaberi, Z.; Myers, J. J.; and ElGawady, M., 2015, “Influence of Near-Surface Mounted (NSM) FRP on the Out-of-Plane Behavior of Reinforced Masonry Walls,” 12th North American Masonry Conference, Denver, CO, 12 pp.

Albert, M. L.; Elwi, A. E.; and Cheng, J. R., 2001, “Strengthening of Unreinforced Masonry Walls Using FRPs,” Journal of Composites for Construction, ASCE, V. 5, No. 2, pp. 76-84. doi: 10.1061/(ASCE)1090-0268(2001)5:2(76)

Barros, J. A.; Dias, S. J.; and Lima, J. L., 2007, “Efficacy of CFRP-Based Techniques for the Flexural and Shear Strengthening of Concrete Beams,” Cement and Concrete Composites, V. 29, No. 3, pp. 203-217. doi: 10.1016/j.cemconcomp.2006.09.001

Barros, J. A., and Kotynia, R., 2008, “Possibilities and Challenges of NSM for the Flexural Strengthening of RC Structures,” Fourth International Conference on FRP Composites in Civil Engineering (CICE2008), Zurich, Switzerland, 6 pp.

De Lorenzis, L., and Nanni, A., 2002, “Bond between Near-Surface Mounted Fiber-Reinforced Polymer Rods and Concrete in Structural Strengthening,” ACI Structural Journal, V. 99, No. 2, Mar.-Apr., pp. 123-132.

De Lorenzis, L.; Nanni, A.; and La Tegola, A., 2000a, “Bond of Near Surface Mounted FRP Rods in Concrete Masonry Units,” Proceedings of the Seventh Annual International Conference on Composites Engineering (ICCE/7), Denver, CO.

De Lorenzis, L.; Tinazzi, D.; and Nanni, A., 2000b, “Near Surface Mounted FRP Rods for Masonry Strengthening: Bond and Flexural Testing,” Proceedings of the International Conference on Composite Engineering, Venice, Italy, 13 pp.

Galati, N.; Tumialan, G.; and Nanni, A., 2006, “Strengthening with FRP Bars of URM Walls Subject to Out-of-Plane Loads,” Construction and Building Materials, V. 20, No. 1-2, pp. 101-110. doi: 10.1016/j.conbuildmat.2005.06.047

Gilstrap, J. M., and Dolan, C. W., 1998, “Out-of-Plane Bending of FRP-Reinforced Masonry Walls,” Composites Science and Technology, V. 58, No. 8, pp. 1277-1284. doi: 10.1016/S0266-3538(98)00007-4

Griffith, M. C.; Kashyap, J.; and Mohamed Ali, M. S., 2013, “Flexural Displacement Response of NSM FRP Retrofitted Masonry Walls,” Construction and Building Materials, V. 49, pp. 1032-1040. doi: 10.1016/j.conbuildmat.2012.06.065

Hamoush, S.; McGinley, M.; Mlakar, P.; and Terro, M. J, 2002, “Out-of-Plane Behavior of Surface-Reinforced Masonry Walls,” Construction and Building Materials, V. 16, No. 6, pp. 341-351. doi: 10.1016/S0950-0618(02)00024-7

Hochwalt, J., and Amrhein, J., 2012, Reinforced Masonry Engineering Handbook, Masonry Institute of America and International Code Council, Torrance, CA.

Konthesingha, K.; Masia, M.; Petersen, R.; and Page, A., 2009, “Bond Behaviour of NSM FRP Strips to Modern Clay Brick Masonry Prisms under Cyclic Loading,” 11th Canadian Masonry Symposium, Toronto, ON, Canada, 10 pp.

Nanni, A., and Tumialan, J. G., 2003, “Fiber-Reinforced Composites for the Strengthening of Masonry Structures,” Structural Engineering International, V. 13, No. 4, pp. 271-278. doi: 10.2749/101686603777964360

Parretti, R., and Nanni, A., 2004, “Strengthening of RC Members Using Near-Surface Mounted FRP Composites: Design Overview,” Advances in Structural Engineering, V. 7, No. 6, pp. 469-483. doi: 10.1260/1369433042863198

Petersen, R. B.; Masia, M. J.; and Seracino, R., 2009, “Bond Behavior of Near-Surface Mounted FRP Strips Bonded to Modern Clay Brick Masonry Prisms: Influence of Strip Orientation and Compression Perpendicular to the Strip,” Journal of Composites for Construction, ASCE, V. 13, No. 3. doi: 10.1061/(ASCE)1090-0268(2009)13:3(169)

Priestley, M. N.; Seible, F.; and Calvi, G. M., 1996, Seismic Design and Retrofit of Bridges, John Wiley & Sons, New York, 704 pp.

Stone, D.; Tumialan, G.; Nanni, A.; and Parretti, R., 2002, “Near-Surface Mounted FRP Reinforcement: Application of an Emerging Technology,” Concrete (London), V. 36, No. 5, pp. 42-44.

Tumialan, G.; Tinazzi, D.; Myers, J.; and Nanni, A., 2000, “Field Evaluation of Unreinforced Masonry Walls Strengthened with FRP Composites Subjected to Out-of-Plane Loading,” 2000 Structures Congress, American Society of Civil Engineers, Philadelphia, PA.

Tumialan, J. G.; Galati, N.; Namboorimadathil, S. M.; and Nanni, A., 2002, “Strengthening of Masonry with FRP Bars,” 3rd International Conference on Composites in Infrastructure (ICCI 2002), San Francisco, CA.

Tumialan, J. G.; Galati, N.; and Nanni, A., 2003, “Fiber-Reinforced Polymer Strengthening of Unreinforced Masonry Walls Subject to Out-of-Plane Loads,” ACI Structural Journal, V. 100, No. 3, May-June, pp. 321-329.

Willis, C.; Kashyap, J.; and Griffith, M., 2009a, “Flexural Behaviour of NSM CFRP Retrofitted Masonry Wallettes under Static and Cyclic Loading,” 9th International Symposium on FRP Reinforcement for Concrete Structures, Sydney, Australia.

Willis, C.; Seracino, R.; and Griffith, M., 2010, “Out-of-Plane Strength of Brick Masonry Retrofitted with Horizontal NSM CFRP Strips,” Engineering Structures, V. 32, No. 2, pp. 547-555. doi: 10.1016/j.engstruct.2009.10.015

Willis, C.; Yang, Q.; Seracino, R.; and Griffith, M., 2009b, “Bond Behaviour of FRP-to-Clay Brick Masonry Joints,” Engineering Structures, V. 31, No. 11, pp. 2580-2587. doi: 10.1016/j.engstruct.2009.06.006


ALSO AVAILABLE IN:

Electronic Structural Journal