Title: Accelerated Mortar Bar Test Precision with Recycled Concrete Aggregate

Author(s): Bryce D. Fiore, Kenneth Gerow, Matthew P. Adams, and Jennifer E. Tanner

Publication: Materials Journal

Volume: 115

Issue: 4

Appears on pages(s): 531-540

Keywords: accelerated mortar bar test; alkali-silica reaction (ASR); precision; recycled concrete aggregate (RCA); variation

DOI: 10.14359/51702186

Date: 7/1/2018

Abstract:
Producing concrete requires considerable quantities of natural aggregates, and contributes to large amounts of solid waste in both production and when removed from service. With many structures reaching the end of their service life, a means of concrete disposal is needed that is both practical and eco-friendly. Reusing concrete waste as recycled concrete aggregate (RCA) in new concrete is a promising solution. However, the current use of RCA is generally limited to backfill and road base. Additionally, alkali-silica reaction (ASR) can pose a substantial obstacle to highly durable concrete and with limited research on ASR behavior in RCA, effective design recommendations are lacking. Current methods of ASR mitigation depend on experimental testing for aggregate classification. Therefore, a multi-laboratory study was done using ASTM C1260 with nine laboratories and 10 operators to determine within- and between-laboratory variation on ASR expansions. The result of this investigation suggests a small change to the existing precision statements of ASTM C1260 to allow the standard to incorporate RCA into the accelerated mortar bar test (AMBT). In addition, testing revealed that expansions using RCA and natural aggregates produced nonreactive or moderately reactive mortar mixtures far more frequently than highly reactive mixtures.

Related References:

1. ASCE, “ASCE’s 2017 Infrastructure Report Card | GPA: D+,” American Society of Civil Engineers, Reston, VA, 2017.

2. Mehta, P. K., “Reducing the Environmental Impact of Concrete,” Concrete International, V. 23, No. 10, Oct. 2001, pp. 61-66.

3. Levy, S. M., and Helene, P., “Durability of Recycled Aggregates Concrete: A Safe Way to Sustainable Development,” Cement and Concrete Research, V. 34, No. 11, 2004, pp. 1975-1980. doi: 10.1016/j.cemconres.2004.02.009

4. Fournier, B., and Berube, M. A., “Alkali-Aggregate Reaction in Concrete: A Review of Basic Concepts and Engineering Implications,” Canadian Journal of Civil Engineering, V. 27, No. 2, 2000, pp. 167-191. doi: 10.1139/l99-072

5. Rajabipour, F.; Giannini, E.; Dunant, C.; Ideker, J.; and Thomas, M., “Alkali-Silica Reaction: Current Understanding of the Reaction Mechanisms and the Knowledge Gaps,” Cement and Concrete Research, V. 76, 2015, pp. 130-146. doi: 10.1016/j.cemconres.2015.05.024

6. Glasser, L. S., and Kataoka, N., “The Chemistry of ‘Alkali-Aggregate’ Reaction,” Cement and Concrete Research, V. 11, No. 1, 1981, pp. 1-9. doi: 10.1016/0008-8846(81)90003-X

7. Stanton, T. E., “Expansion of Concrete through Reaction between Cement and Aggregate,” Proceedings of the American Society of Civil Engineers, V. 66, 1940, pp. 1781-1810.

8. Mehta, P. K., “Greening of the Concrete Industry for Sustainable Development,” Concrete International, V. 24, No. 7, July 2002, pp. 23-38.

9. IEA, WBCSD, Carbon Emissions Reductions up to 2050, Energy Agency (IEA), Paris, France, 2009.

10. Meyer, C., “The Greening of the Concrete Industry,” Cement and Concrete Composites, V. 31, No. 8, 2009, pp. 601-605. doi: 10.1016/j.cemconcomp.2008.12.010

11. Meyer, C., The Economics of Recycling in the US Construction Industry, Taylor & Francis, Coventry, UK, 2007.

12. Rao, A.; Jha, K. N.; and Misra, S., “Use of Aggregates from Recycled Construction and Demolition Waste in Concrete,” Resources, Conservation and Recycling, V. 50, No. 1, 2007, pp. 71-81. doi: 10.1016/j.resconrec.2006.05.010

13. Hansen, T. C., and Lauritzen, E. K., “Concrete Waste in a Global Perspective,” Recycling Concrete and Other Materials for Sustainable Development, SP-219, T. C. Liu and C. Meyer, eds., American Concrete Institute, Farmington Hills, MI, 2004, pp. 35-46.

14. Adams, M. P.; Jones, A.; Beauchemin, S.; Johnson, R.; Fournier, B.; Shehata, M.; Tanner, J. E.; and Ideker, J. H., “Applicability of the Accelerated Mortar Bar Test for Alkali Silica Reactivity of Recycled Concrete Aggregates,” Advances in Civil Engineering Materials, V. 2, No. 1, 2013, pp. 78-96. doi: 10.1520/ACEM20120030

15. Gao, X. X.; Cyr, M.; Multon, S.; and Sellier, A., “A Comparison of Methods for Chemical Assessment of Reactive Silica in Concrete Aggregates by Selective Dissolution,” Cement and Concrete Composites, V. 37, 2013, pp. 82-94. doi: 10.1016/j.cemconcomp.2012.12.002

16. Mukhopadhyay, A. K., “An Effective Approach to Utilize Recycled Aggregates (RAs) from Alkali-Silica Reaction (ASR) Affected Portland Cement Concrete,” Woodhead Publishing Series in Civil and Structural Engineering, 2013, pp. 555-568.

17. Farny, J. A., and Kerkhoff, B., “Diagnosis and Control of Alkali-Aggregate Reactions in Concrete,” Portland Cement Association, Skokie, IL, 2007.

18. Li, X., and Gress, D. L., “Mitigating Alkali-Silica Reaction in Concrete Containing Recycled Concrete Aggregate,” Transportation Research Record: Journal of the Transportation Research Board, V. 1979, 2006, pp. 30-35. doi: 10.3141/1979-06

19. Shehata, M. H.; Christidis, C.; Mikhaiel, W.; Rogers, C.; and Lachemi, M., “Reactivity of Reclaimed Concrete Aggregate Produced from Concrete Affected by Alkali-Silica Reaction,” Cement and Concrete Research, V. 40, No. 4, 2010, pp. 575-582. doi: 10.1016/j.cemconres.2009.08.008

20. Lu, D.; Fournier, B.; and Grattan-Bellew, P. E., “Evaluation of Accelerated Test Methods for Determining Alkali-Silica Reactivity of Concrete Aggregates,” Cement and Concrete Composites, V. 28, No. 6, 2006, pp. 546-554. doi: 10.1016/j.cemconcomp.2006.03.001

21. Tabsh, S. W., and Abdelfatah, A. S., “Influence of Recycled Concrete Aggregates on Strength Properties of Concrete,” Construction and Building Materials, V. 23, No. 2, 2009, pp. 1163-1167. doi: 10.1016/j.conbuildmat.2008.06.007

22. Tam, V., “Comparing the Implementation of Concrete Recycling in the Australian and Japanese Construction Industries,” Journal of Cleaner Production, V. 17, No. 7, 2009, pp. 688-702. doi: 10.1016/j.jclepro.2008.11.015

23. USGS, “Fact Sheet FS-181-99: Recycled Aggregates—Profitable Resource Conservation,” U.S. Geological Survey, Denver, CO, 2000, 2 pp.

24. Ideker, J. H.; Adams, M. P.; Tanner, J. E.; and Jones, A., “Durability Assessment of Recycled Concrete Aggregates for Use in New Concrete-Phase II,” Oregon Transportation Research and Education Consortium, 2014, pp. 1-110.

25. Osmani, M., “Construction Waste Minimization in the UK: Current Pressures for Change and Approaches,” Procedia: Social and Behavioral Sciences, V. 40, 2012, pp. 37-40. doi: 10.1016/j.sbspro.2012.03.158

26. Jin, R., and Chen, Q., “Investigation of Concrete Recycling in the U.S. Construction Industry,” Procedia Engineering, V. 118, 2015, pp. 894-901. doi: 10.1016/j.proeng.2015.08.528

27. Sagoe-Crentsil, K. K.; Brown, T.; and Taylor, A. H., “Performance of Concrete Made with Commercially Produced Coarse Recycled Concrete Aggregate,” Cement and Concrete Research, V. 31, No. 5, 2001, pp. 707-712. doi: 10.1016/S0008-8846(00)00476-2

28. Kou, S. C.; Poon, C. S.; and Etxeberria, M., “Influence of Recycled Aggregates on Long Term Mechanical Properties and Pore Size Distribution of Concrete,” Cement and Concrete Composites, V. 22, No. 2, 2011, pp. 286-291. doi: 10.1016/j.cemconcomp.2010.10.003

29. Malhotra, V. M., “Recycled Concrete—A New Aggregate,” Canadian Journal of Civil Engineering, V. 5, No. 1, 1978, pp. 42-52. doi: 10.1139/l78-006

30. Adams, M. P.; Fu, T.; Cabrera, A. G.; Morales, M.; Ideker, J. H.; and Isgor, O. B., “Cracking Susceptibility of Concrete Made with Coarse Recycled Concrete Aggregates,” Construction and Building Materials, V. 102, No. 1, 2016, pp. 802-810. doi: 10.1016/j.conbuildmat.2015.11.022

31. Marie, I., and Quiasrawi, H., “Close-Loop Recycling of Recycled Concrete Aggregates,” Journal of Cleaner Production, V. 37, 2012, pp. 243-248. doi: 10.1016/j.jclepro.2012.07.020

32. Berube, M. A.; Duchesne, J.; Dorion, J. F.; and Rivest, M., “Laboratory Assessment of Alkali Contributions by Aggregates to Concrete And Application to Concrete Structures Affected by Alkali-Silica Reactivity,” Cement and Concrete Research, V. 32, No. 8, 2002, pp. 1215-1227. doi: 10.1016/S0008-8846(02)00766-4

33. Berube, M. A., and Fournier, B., “Canadian Experience with Testing for Alkali-Aggregate Reactivity in Concrete,” Cement and Concrete Composites, V. 15, No. 1-2, 1993, pp. 27-47. doi: 10.1016/0958-9465(93)90037-A

34. Thomas, M.; Fournier, B.; Folliard, K.; Ideker, J.; and Shehata, M., “Test Methods for Evaluating Preventive Measures for Controlling Expansion due to Alkali-Silica Reaction in Concrete,” International Center for Aggregates Research, Austin, TX, 2006.

35. ASTM C1260-14, “Standard Test Method for Determining the Potential Alkali-Silica Reaction of Combinations of Cementitious Materials and Aggregate (Accelerated Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2014, 5 pp.

36. Johnson, R., and Shehata, M. H., “The Efficacy of Accelerated Test Methods to Evaluate Alkali Silica Reactivity of Recycled Concrete Aggregates,” Construction and Building Materials, V. 112, 2016, pp. 518-528. doi: 10.1016/j.conbuildmat.2016.02.155

37. Etxeberria, M., and Vázquez, E., “Alkali Silica Reaction in Concrete Induced by Mortar Adhered to Recycled Aggregate,” Materiales de Construcción, V. 60, No. 297, 2010, 12 pp.

38. Kimble, M.; Fertig, R.; Hacker, D.; and Tanner, J. E., “Evaluating the Risk of Alkali-Silica Reaction in Wyoming: Continued Evaluation of Field Specimens and Proposed Mitigation Strategies,” FHWA-WY-15/04F, Federal Highway Administration, Washington, DC, 2015, pp. 1-211.

39. ASTM C150/C150M-16, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2016, 10 pp.

40. ACI Committee 211, “Report on Alkali-Aggregate Reactivity (ACI 221.R-98) (Reapproved 2008),” American Concrete Institute, Farmington Hills, MI, 2008, 31 pp.

41. Ideker, J. H.; Bentivegna, A. F.; Folliard, K. J.; and Juenger, M. C. G., “Do Current Laboratory Test Methods Accurately Predict Alkali-Silica Reactivity?” ACI Materials Journal, V. 109, No. 4, July-Aug. 2012, pp. 395-402.

42. ASTM C1293-08b, “Standard Test Method for Determination of Length Change of Concrete Due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2008, 7 pp.

43. ASTM C305-14, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA, 2014, 3 pp.

44. Thomas, M. D.; Fournier, B.; and Folliard, K. J., “Selecting Measures to Prevent Deleterious Alkali-Silica Reaction in Concrete: Rationale for the AASHTO PP65 Prescriptive Approach,” U.S. Department of Transportation Federal Highway Administration, Washington, DC, 2012.

45. Rogers, C. A., “Multi-Laboratory Study of the Accelerated Mortar Bar Test (ASTM C1260) for Alkali Silica Reaction,” Cement and Concrete Research Aggregates, V. 21, No. 2, 1999, pp. 185-194. doi: 10.1520/CCA10432J

46. Poon, C. S.; Shui, Z. H.; Lam, L.; Fok, H.; and Kou, S. C., “Influence of Moisture States of Natural and Recycled Aggregates on the Slump and Compressive Strength of Concrete,” Cement and Concrete Research, V. 34, No. 1, 2004, pp. 31-36. doi: 10.1016/S0008-8846(03)00186-8

47. Tam, V. W. Y.; Gao, X. F.; Tam, C. M.; and Chan, C. H., “New Approach in Measuring Water Absorption of Recycled Aggregates,” Construction and Building Materials, V. 22, No. 3, 2008, pp. 364-369. doi: 10.1016/j.conbuildmat.2006.08.009

48. Scott, H. C. I., and Gress, D. L., “Mitigating Alkali Silica Reaction in Recycled Concrete,” Recycling Concrete and Other Materials for Sustainable Development, American Concrete Institute, V. 219, 2004, pp. 61-76.

49. Ferreira, L.; de Brito, J.; and Barra, M., “Influence of the Pre-Saturation of Recycled Coarse Concrete Aggregates on Concrete Properties,” Magazine of Concrete Research, V. 63, No. 8, 2011, pp. 617-627. doi: 10.1680/macr.2011.63.8.617

50. Delobel, F.; Bulteel, D.; Mechling, J. M.; Lecomte, A.; Cyr, M.; and Rémond, S., “Application of ASR Tests to Recycled Concrete Aggregates: Influence of Water Absorption,” Construction and Building Materials, V. 124, 2016, pp. 714-721. doi: 10.1016/j.conbuildmat.2016.08.004

51. Philleo, R. E., “Establishing Specification Limits for Materials,” Cement, Concrete and Aggregates, V. 1, No. 2, 1979, pp. 83-87. doi: 10.1520/CCA10409J

52. Ullman, N., “What Are Repeatability and Reproducibility? Part 2: The E11 Viewpoint,” ASTM Standardization News, ASTM International, West Conshohocken, PA, 2009, https://www.astm.org/SNEWS/MJ_2009/datapoints_mj09.html. (last accessed July 19, 2018)

53. ASTM C670-15, “Standard Practice for Preparing Precision and Bias Statements for Test Methods for Construction Materials,” ASTM International, West Conshohocken, PA, 2015, 9 pp.

54. ASTM E177-14, “Standard Practice for Use of the Terms Precision and Bias in ASTM Test Methods,” ASTM International, West Conshohocken, PA, 2014, 9 pp.

55. Miller, I., and Miller, M., John E. Freund’s ‘Mathematical Statistics With Applications’, eighth edition, Pearson Education, London, UK, 2014.

56. Lau, A., “What Are Repeatability and Reproducibility? Part 1: A D02 Viewpoint for Laboratories,” ASTM Standardization News, ASTM International, West Conshohocken, PA, 2009, https://www.astm.org/SNEWS/MA_2009/datapoints_ma09.html. (last accessed July 19, 2018)

57. Shehata, M. H.; Christidis, C.; Mikhaiel, W.; Rogers, C.; and Lachemi, M., “Reactivity of Reclaimed Concrete Aggregate Produced from Concrete Affected by Alkali-Silica Reaction,” Cement and Concrete Research, V. 40, No. 4, 2010, pp. 575-582. doi: 10.1016/j.cemconres.2009.08.008


ALSO AVAILABLE IN:

Electronic Materials Journal