Lab and Field Data for Assessing the Impact of "Green" Concrete Mixtures on Building Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Lab and Field Data for Assessing the Impact of "Green" Concrete Mixtures on Building Construction

Author(s): Ward R. Malisch and Bruce A. Suprenant

Publication: CRC

Volume:

Issue:

Appears on pages(s):

Keywords: green, green concrete, supplementary cementitious material, SCM, portland cement

DOI:

Date: 12/1/2013

Abstract:
The Charles Pankow Foundation provided major funding to the American Society of Concrete Contractors Education, Research, and Development Foundation for development of “Assessing the Impact of “Green” Concrete Mixtures on Building Construction." The term “green” concrete in this context refers especially to concrete containing supplementary cementitious materials (SCMs) that replace relatively large amounts of portland cement. In preparation for writing the Guide, a laboratory and field testing program was conducted to provide data that would supplement and illustrate construction challenges of green concrete that had been experienced on specific projects. This report summarizes the testing program results and includes all of the raw data that comprise the results.