315-18: Guide to Presenting Reinforcing Steel Design Details

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: 315-18: Guide to Presenting Reinforcing Steel Design Details

Author(s): ACI Committee 315

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords: concrete structures; design details; detailing; engineering drawings; fabrication details; placing drawings; reinforcement; reinforcing steel; tolerances.

DOI:

Date: 1/26/2018

Abstract:
This document guides designers of concrete structures how to determine information and design details that are required to prepare reinforcing steel fabrication details and placing drawings. The guide stresses the importance of this information to ensure that the reinforcing steel detailer effectively and accurately captures the intent of the designer, presenting it in a manner that is clear and unambiguous to the reinforcing steel fabricator and placer. Recommendations are also provided concerning the review of placing drawings.