Thermomechanical Relaxation of Reinforced Concrete Beams Strengthened with Carbon Fiber-Reinforced Polymer

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thermomechanical Relaxation of Reinforced Concrete Beams Strengthened with Carbon Fiber-Reinforced Polymer

Author(s): Yail J. Kim and Abdulaziz Alqurashi

Publication: Structural Journal

Volume: 115

Issue: 1

Appears on pages(s): 259-268

Keywords: carbon fiber-reinforced polymer (CFRP); relaxation; retrofit; strengthening; thermal

DOI: 10.14359/51701091

Date: 1/1/2018

Abstract:
This paper presents the behavior of reinforced concrete beams strengthened with carbon fiber reinforced polymer (CFRP) sheets subjected to relaxation induced by thermal and mechanical loadings that are applied simultaneously (thermomechanical loading). The range of elevated temperatures varies from 75 to 150°C (167 to 302°F) and the mechanical load represents a typical service condition (60% of the strengthened beam’s capacity at 25°C [77°F]), both of which are sustained for 30- to 75-minute periods. The heat conduction of the beams is measured by an infrared imaging technique to understand their thermal responses. Upon completion of the thermomechanical relaxation test, all beams are loaded to failure for residual capacity investigations. The progression of thermal loading across the CFRP-concrete interface exhibits a so-called latent heat effect that takes place with thermal conduction along the interface. During residual testing, the degraded interface reveals partial debonding that accompanies the retraction of CFRP strains. Thermomechanical relaxation influences the residual capacity, load displacement, and interfacial cracking patterns of the strengthened beams. According to analytical modeling, the elastic modulus of CFRP and the magnitude of a mechanical load affect the degree of thermomechanical relaxation. A design factor is proposed based on multiple regression to quantify the implications of thermomechanical relaxation for CFRP-strengthened beams.

Related References:

1. Williams, B.; Kodur, V.; Green, M. F.; and Bisby, L., “Fire Endurance of Fiber-Reinforced Polymer Strengthened Concrete T-Beams,” ACI Structural Journal, V. 105, No. 1, Jan.-Feb. 2008, pp. 60-67.

2. Kodur, V. K. R., and Yu, B., “Rational Approach for Evaluating Fire Resistance of FRP-Strengthened Concrete Beams,” Journal of Composites for Construction, ASCE, V. 20, No. 6, 2016, 04016041. doi: 10.1061/(ASCE)CC.1943-5614.0000697

3. Hu, W., Polymer Physics: A Molecular Approach, Springer, Berlin, Germany, 2013.

4. Gamage, J. C. P. H.; Al-Mahaidi, R.; and Wong, M. B., “Bond Characteristics of CFRP Plated Concrete Members under Elevated Temperatures,” Composite Structures, V. 75, No. 1-4, 2006, pp. 199-205. doi: 10.1016/j.compstruct.2006.04.068

5. Leone, M.; Matthys, S.; and Aiello, M. A., “Effect of Elevated Service Temperature on Bond between FRP EBR Systems and Concrete,” Composites. Part B, Engineering, V. 40, No. 1, 2009, pp. 85-93. doi: 10.1016/j.compositesb.2008.06.004

6. Tan, K.-H.; Toh, W.-S.; Huang, Z.-F.; and Phng, G. H., “Structural Responses of Restrained Steel Columns at Elevated Temperatures,” Engineering Structures, V. 29, No. 8, 2007, pp. 1641-1652. doi: 10.1016/j.engstruct.2006.12.005

7. Sadaoui, A., and Khennane, A., “Effect of Transient Creep on the Behaviour of Reinforced Concrete Columns in Fire,” Engineering Structures, V. 31, No. 9, 2009, pp. 2203-2208. doi: 10.1016/j.engstruct.2009.04.005

8. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 76 pp.

9. Kraus, H., Creep Analysis, John Wiley & Sons, New York, 1980.

10. Kim, Y. J.; Hmidan, A.; and Choi, K.-K., “Residual Behavior of Shear-Repaired Concrete Beams Using CFRP Sheets Subjected to Elevated High Temperatures,” Journal of Composites for Construction, ASCE, V. 16, No. 3, 2012, pp. 253-264. doi: 10.1061/(ASCE)CC.1943-5614.0000244

11. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

12. ACI Committee 216, “Guide for Determining the Fire Endurance of Concrete Elements (ACI 216R-89) (Reapproved 2001),” American Concrete Institute, Farmington Hills, MI, 1989, 48 pp.

13. Mitchell, M., An Introduction to Genetic Algorithms, MIT Press, Cambridge, MA. 1998.

14. Casalini, R.; Fioretto, D.; Livi, A.; Lucchesi, M.; and Rolla, P. A., “Influence of the Glass Transition on the Secondary Relaxation of an Epoxy Resin,” Physical Review B: Condensed Matter and Materials Physics, V. 56, No. 6, 1997, pp. 3016-3021. doi: 10.1103/PhysRevB.56.3016


ALSO AVAILABLE IN:

Electronic Structural Journal