Title: Concrete Q&A: Epoxy-Coated Reinforcement and Cover Depth Against Ground

Author(s):

Publication: Concrete International

Volume: 40

Issue: 1

Appears on pages(s): 63-64

Keywords:

DOI: 10.14359/51702021

Date: 1/1/2018

Abstract:

Table 20.6.1.3.1 of ACI 318-141

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

2. Standard Specifications No. 23, “Standard Building Regulations for the Use of Reinforced Concrete,” American Concrete Institute, Farmington Hills, MI, 1920, pp. 283-302.

3. MacGregor, J.G., Reinforced Concrete: Mechanics and Design, third edition, Prentice Hall, Upper Saddle River, NJ, 1997, 939 pp.