Use of Zeolitized Coal Fly Ash as Main Component in Panels with High Fire Resistance

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Zeolitized Coal Fly Ash as Main Component in Panels with High Fire Resistance

Author(s): C. Leiva, C. Arenas, L. F. Vilches, F. Arroyo, Y. Luna-Galiano, R. Villegas, and C. Fernández- Pereira

Publication: Materials Journal

Volume: 115

Issue: 3

Appears on pages(s): 393-399

Keywords: fire resistance; leaching; mechanical strength; radiological properties; zeolitized fly ashes

DOI: 10.14359/51702009

Date: 5/1/2018

Abstract:
In the present work, coal fly ashes from a Spanish coal-fired power plant were used to synthesize zeolite using an alkaline treatment. The feasibility of making highly fire-insulated panels using these zeolitized fly ashes was examined. The panels were prepared using zeolitized fly ashes as the main component (50, 60, and 70% by weight) combined with gypsum, silica fume (4.5% by weight, constant), and glass fiber (9.5% by weight, constant). The manufactured panels had great water retention capacity and, consequently, showed up to 30% greater insulating properties compared to commercial gypsum panels. It was found that compression and bending strengths diminished as the proportion of zeolitized fly ashes increased, and the panels did not present any leachability of heavy metals or radiological problems. The panels developed with zeolitized fly ashes could potentially be useful as a component in construction materials for passive fire protection in doors and firewalls in buildings and industrial installations.

Related References:

1. Blissett, R. S., and Rowson, N. A., “A Review of the Multi-­Component Utilisation of Coal Fly Ash,” Fuel, V. 97, 2012, pp. 1-23. doi: 10.1016/j.fuel.2012.03.024

2. American Coal Ash Association (ACAA), “Beneficial Use of Coal Combustion Products: An American Recycling Success Story,” 2016, https://www.acaa-usa.org/Portals/9/Files/PDFs/ACAA-Brochure-Web.pdf. (last accessed July 14, 2017)

3. Madurwar, M. V.; Mandavgane, S. A.; and Raleagonkar, R., “Development and Feasibility Analysis of Bagasse Ash Bricks,” Journal of Energy Engineering, V. 141, No. 3, 2014, pp. 1-10.

4. Querol, X.; Plana, F.; Alastuey, A.; and López-Soler, A., “Synthesis of Na-Zeolites from fly Ash,” Fuel, V. 76, No. 8, 1997, pp. 793-799. doi: 10.1016/S0016-2361(96)00188-3

5. Koshy, N., and Singh, D. N., “Fly Ash Zeolites for Water Treatment Applications,” Journal of Environmental Chemical Engineering, V. 4, No. 2, 2016, pp. 1460-1472. doi: 10.1016/j.jece.2016.02.002

6. Shaila, K.; Nisha, D.; Pralhad, P.; and Deepa, P., “Zeolite Synthesis Strategies from Coal Fly Ash: A Comprehensive Review of Literature,” International Research Journal in Environment Sciences, V. 4, No. 3, Mar. 2015, pp. 93-99.

7. Liu, Y.; Yan, C.; Zhang, Z.; Li, L.; Wang, H.; and Pu, S., “One-Step Fabrication of Novel Porous and Permeable Self-Supporting Zeolite Block from Fly Ash,” Materials Letters, V. 196, 2017, pp. 328-331. doi: 10.1016/j.matlet.2017.03.097

8. Fukasawa, T.; Karisma, A. D.; Shibata, D.; Huang, A. N.; and Fukui, K., “Synthesis of Zeolite from Coal Fly Ash by Microwave Hydrothermal Treatment with Pulverization Process,” Advanced Powder Technology, V. 28, No. 3, 2017, pp. 798-804. doi: 10.1016/j.apt.2016.12.006

9. Deng, L.; Xu, Q.; and Wu, H., “Synthesis of Zeolite-like Material by Hydrothermal and Fusion Methods Using Municipal Solid Waste Fly Ash,” Procedia Environmental Sciences, V. 31, 2016, pp. 662-667. doi: 10.1016/j.proenv.2016.02.122

10. Ding, J.; Fu, Y. Y.; and Beaudoin, J. J., “Effect of Different Zeolites on Conversion-Prevention in High-Alumina Cement Products,” ACI Materials Journal, V. 94, No. 3, May-June 1997, pp. 220-226.

11. Moreno, N.; Querol, X.; Ayora, C.; Pereira, C. F.; and Janssen-Jurkovicová, M., “Utilization of Zeolites Synthesized from Coal Fly Ash for the Purification of Acid Mine Waters,” Environmental Science & Technology, V. 35, No. 17, 2001, pp. 3526-3534. doi: 10.1021/es0002924

12. Vilches, L. F.; Leiva, C.; Vale, J.; Olivares, J.; and Fernández Pereira, C., “Coal Fly Ash-Containing Sprayed Mortar for Passive Fire Protection of Steel Sections,” Materiales de Construcción, V. 55, 2005, pp. 25-37. doi: 10.3989/mc.2005.v55.i279.196

13. Li, J.; Zhuang, X.; Leiva, C.; Cornejo, A.; Font, O.; Querol, X.; Moreno, N.; Arenas, C.; and Fernández-Pereira, C., “Potential Utilization of FGD Gypsum and Fly Ash from a Chinese Power Plant for Manufacturing Fire-Resistant Panels,” Construction and Building Materials, V. 95, No. 12, 2015, pp. 910-921. doi: 10.1016/j.conbuildmat.2015.07.183

14. Leiva, C.; Solís-Guzmán, J.; Marrero, M.; and García Arenas, C., “Recycled Blocks with Improved Sound and Fire Insulation Containing Construction and Demolition Waste,” Waste Management (New York, N.Y.), V. 33, No. 3, 2013, pp. 663-671. doi: 10.1016/j.wasman.2012.06.011

15. Luna-Galiano, Y.; Cornejo, A.; Leiva, C.; Vilches, L. F.; and Fernández-Pereira, C., “Properties of Fly Ash and Metakaolin Based Geopolymer Panels under Fire Resistance Tests,” Materiales de Construcción, V. 65, No. 319, 2015, pp. 1-13. doi: 10.3989/mc.2015.06114

16. Querol, X.; Umaña, J. C.; Plana, F.; Alastuey, A.; López-Soler, A.; Medinaceli, A.; Valero, A.; Domingo, M. J.; and Garcia-Rojo, E., “Synthesis of Zeolites from Fly Ash at Pilot Plant Scale. Examples of Potential Environmental Applications,” Fuel, V. 80, No. 6, 2001, pp. 857-865. doi: 10.1016/S0016-2361(00)00156-3

17. EN 13263-1, “Silica Fume for Concrete – Part 1: Definitions, Requirements and Conformity Criteria,” European Committee for Standardization, Brussels, Belgium, 2009, 24 pp.

18. Hasan-Nattaj, F., and Nematzadeh, M., “The Effect of Forta-Ferro and Steel Fibers on Mechanical Properties of High-Strength Concrete with and without Silica Fume and Nano-Silica,” Construction and Building Materials, V. 137, No. 15, 2017, pp. 557-572. doi: 10.1016/j.conbuildmat.2017.01.078

19. Leiva, C.; Vilches, L. F.; Vale, J.; and Fernández-Pereira, C., “Fire Resistance of Biomass Ash Panels Used for Internal Partitions in Buildings,” Fire Safety Journal, V. 44, No. 4, 2009, pp. 622-628. doi: 10.1016/j.firesaf.2008.12.005

20. EN13279-2, “Gypsum Binders and Gypsum Plasters — Part 2: Test Methods,” European Committee for Standardization, Brussels, Belgium, 2014.

21. ASTM E761-92(2011), “Standard Test Method for Compressive Strength of Sprayed Fire-Resistive Material Applied to Structural Members,” ASTM International, West Conshohocken, PA, 2011, 3 pp.

22. ASTM C348-14, “Standard Test Method for Flexural Strength of Hydraulic-Cement Mortars,” ASTM International, West Conshohocken, PA, 2014, 6 pp.

23. EN 1363-1, “Fire Resistance Test. Part 1: General Requirements,” European Committee for Standardization, Brussels, Belgium, 2015, 54 pp.

24. EN 12457-4, “Characterization of Waste: Leaching. Compliance Test for Leaching of Granular Waste Material and Sludges. Part 2: One Stage Batch Test at a Liquid to Solid Ratio of 10 l/kg for Materials with Particle Size below 10 mm (without or with Size Reduction),” European Committee for Standardization, Brussels, Belgium, 2003, 34 pp.

25. EN 12859, “Gypsum Blocks. Definitions, Requirements and Test Methods,” European Committee for Standardization, Brussels, Belgium, 2012, 38 pp.

26. Mei, X. P.; Zheng, H. W.; Shao, H. S.; Qiu, G. X.; Long, J. L.; Yu, C. T.; and Lin, L. H., “Alkali Fusion of Bentonite to Synthesize One-Part Geopolymeric Cements Cured at Elevated Temperature by Comparison with Two-Part Ones,” Construction and Building Materials, V. 130, No. 15, 2017, pp. 103-112.

27. Girskas, G., and Skripkiūnas, G., “The Effect of Synthetic Zeolite on Hardened Cement Paste Microstructure and Freeze-Thaw Durability of Concrete,” Construction and Building Materials, V. 142, 2017, pp. 117-127. doi: 10.1016/j.conbuildmat.2017.03.056

28. EN 13279-1, “Gypsum Binders and Gypsum Plasters. Part 1. Definitions and Requirements,” European Committee for Standardization, Brussels, Belgium, 2009, 24 pp.

29. “Order on Valorization of Slags of 15 February 1996,” Generalitat de Catalunya DO (1996) 2181, 3 pp.

30. EULFD, “European Landfill Directive 1999/31/EC of 19 December 2002 Establishing Criteria and Procedures for the Acceptance of Waste at Landfills Pursuant to Article 16 of and Annex II to Directive 1999/31/EC,” 2002, 19 pp.

31. Council Directive, 2013/59/Euratom of 5 Dec. 2013 Laying Down Basic Safety Standards for Protection against the Dangers Arising from Exposure to Ionising Radiation, and Repealing Directives 89/618/Euratom, 90/641/Euratom, 96/29/Euratom, 97/43/Euratom and 2003/122/Euratom. L13, vol. 57. ISSN 1977e0677, 2014, 13 pp.

32. “Recommendations for the Implementation of Title VII of the European Basic Safety Standards Directive (BSS) Concerning Significant Increase in Exposure due to Natural Radiation Sources,” European Commission Radiation Protection 88, 1997, 40 pp.

33. Ignjatović, I.; Sas, Z.; Dragaš, J.; Somlai, J.; and Kovács, T., “Radiological and Material Characterization of High Volume Fly Ash Concrete,” Journal of Environmental Radioactivity, V. 168, 2017, pp. 38-45. doi: 10.1016/j.jenvrad.2016.06.021

34. “Radiological Protection Principles Concerning the Natural Radioactivity of Building Materials,” European Commission Radiation Protection 112, 1999, 16 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal