A DEVELOPMENT OF COMPRESSIVE STRENGTH OF CONCRETE FROM A BINDER OF BOTTOM ASH AND CALCIUM CARBIDE RESIDUE

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A DEVELOPMENT OF COMPRESSIVE STRENGTH OF CONCRETE FROM A BINDER OF BOTTOM ASH AND CALCIUM CARBIDE RESIDUE

Author(s): Penpichcha Khongpermgoson, Akkadath Abdulmatin, Weerachart Tangchirapat, Chai Jaturapitakkul

Publication: TCA

Volume: 4

Issue: 1

Appears on pages(s): 11-19

Keywords: Binder, bottom ash, calcium carbide residue, concrete

DOI:

Date: 1/1/2016

Abstract:
In this study, two waste materials, calcium carbide residue and bottom ash, were used as a binder in concrete. Bottom ash from the Mae Moh power plant in Lampang province was mixed with calcium carbide residue, a waste obtained from an acetylene gas production industry in Samutsakorn province. The mixture was used as a binder for casting concrete. This paper focused on the development of compressive strength of the concrete made from the two waste materials to replace cement in concrete. Also, the cement not exceeding 55 kg/m3 was used to promote and increase the compressive strength of concrete. The results demonstrated that the compressive strengths of concrete without cement were as high as 29.7 and 36.8 MPa at 28 days and 90 days, respectively. Also, the adding 55 kg/m3of cement in the concrete mixture produced the compressive strength of 44.3 and 51.4 MPa at 28 and 90 days, respectively. For cement concrete to have the compressive strength of 47 MPa at 28 days, the use of cement in the mixture of 450 kg/m3 was needed. The results also illustrated that the use of concrete made from calcium carbide residue and bottom ash as a binder provided a satisfactory compressive strength and also reduced the use of cement in concrete mixture..


Thailand Concrete Association, International Partner Access

View Resource »