PREDICTION OF WATER TRANSPORT IN CONCRETE WITH AID OF EXPERIMENT INVESTIGATIONS AND DEVELOPED MOISTURE MEASUREMENT METHOD

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: PREDICTION OF WATER TRANSPORT IN CONCRETE WITH AID OF EXPERIMENT INVESTIGATIONS AND DEVELOPED MOISTURE MEASUREMENT METHOD

Author(s): Parnthep Julnipitawong and Lutz Franke

Publication: TCA

Volume: 1

Issue: 2

Appears on pages(s): 30-34

Keywords: Water transport, Microwave

DOI:

Date: 6/1/2013

Abstract:
The developed moisture transport model is introduced in forms of water vapor transport described by Fick’s diffusion and liquid water transport described by Darcy’s law. The transport models are evaluated by comparing with the experiment results of concrete samples subjected to specific studied boundary conditions and measured by microwave based and traditional methods.