Title: CP-1 36th Edition: Technician Workbook for Concrete Field Testing Technician—Grade I

Author(s):

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 12/7/2017

Abstract:
A study guide for the examinee, this workbook provides information and instructional material on the required ASTM testing procedures. ASTM Standards included are: C1064/C1064M–12, C172/C172M–14a, C143/C143M–15a, C138/C138M–17a, C231/C231M–17a, C173/C173M–16, and C31/C31M–17. ASTM C29/C29M and ASTM C94/C94M are included as additional resources.