Aggregate Correction Factors for Concrete Elastic Modulus Prediction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Aggregate Correction Factors for Concrete Elastic Modulus Prediction

Author(s): Caitlin M. Tibbetts, Michael C. Perry, Christopher C. Ferraro, and H. R. (Trey) Hamilton

Publication: Structural Journal

Volume: 115

Issue: 4

Appears on pages(s): 931-940

Keywords: aggregate correction factor; coarse aggregate; compressive strength; limerock; modulus of elasticity; structural design

DOI: 10.14359/51701914

Date: 7/1/2018

Abstract:
The structural design of concrete is typically based on service limit states and uses the modulus of elasticity as a design parameter. However, the modulus of elasticity of concrete used for the design of structures is typically determined indirectly using specified compressive strength. This research investigated the differences between the physical and empirically based relationships of the modulus of elasticity and compressive strength of concrete. Concrete incorporating various types of coarse aggregate was evaluated with particular emphasis on limestone from Florida formations, better known as limerock. The goal of this research was to establish the accuracy of coarse aggregate correction factors used for predicting the modulus of elasticity of concrete. It was found that a value of 1.0, rather than 0.9, was appropriate for the correction factor for Florida limerock; the current structural design guidelines used by the Florida Department of Transportation have revised the specifications to reflect this finding.

Related References:

1. Alexander, M., and Milne, T., “Influence of Cement Blend and Aggregate Type on the Stress-Strain Behavior and Elastic Modulus of Concrete,” ACI Materials Journal, V. 92, No. 3, May-June 1995, pp. 227-235.

2. Beshr, H.; Almusallam, A.; and Maslehuddin, M., “Effect of Coarse Aggregate Quality on the Mechanical Properties of High Strength Concrete,” Construction and Building Materials, V. 17, No. 2, 2002, pp. 97-103. doi: 10.1016/S0950-0618(02)00097-1

3. Gutierrez, P., and Canovas, M., “The Modulus of Elasticity of High Performance Concrete,” Materials and Structures, V. 28, No. 10, 1995, pp. 559-568. doi: 10.1007/BF02473187

4. Aslani, F., and Nejadi, S., “Mechanical Properties of Conventional and Self-Compacting Concrete: An Analytical Study,” Construction and Building Materials, V. 36, 2012, pp. 330-347. doi: 10.1016/j.conbuildmat.2012.04.034

5. Beushausen, H., and Dittmer, T., “The Influence of Aggregate Type on the Strength and Elastic Modulus of High Strength Concrete,” Construction and Building Materials, V. 74, 2015, pp. 132-139. doi: 10.1016/j.conbuildmat.2014.08.055

6. Kockal, N., “Validity and Reliability of Estimated Modulus of Elasticity of Cementitious Materials,” IOP Conference Series. Materials Science and Engineering, V. 103, 2015, p. 012024 doi: 10.1088/1757-899X/103/1/012024

7. Tomosawa, F., and Noguchi, T., “Relationship between Compressive Strength and Modulus of Elasticity of High-Strength Concrete,” Proceedings of the Third International Symposium on Utilization of High-Strength Concrete, V. 2, 1993, pp. 1247–1254.

8. Yıldırım, H., and Sengul, O., “Modulus of Elasticity of Substandard and Normal Concretes,” Construction and Building Materials, V. 25, No. 4, 2011, pp. 1645-1652. doi: 10.1016/j.conbuildmat.2010.10.009

9. Wu, K.; Chen, B.; Yao, W.; and Zhang, D., “Effect of Coarse Aggregate Type on Mechanical Properties of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 10, 2001, pp. 1421-1425. doi: 10.1016/S0008-8846(01)00588-9

10. Tyner, M., “The Effect of Moisture on the Thermal Conductivity of Limerock Concrete,” ACI Journal Proceedings, V. 43, No. 9, Sept. 1946, pp. 9-18.

11. Structures Design Guidelines, Florida Department of Transportation, Tallahassee, FL, 2016, 332 pp.

12. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

13. ACI Committee 435, “Control of Deflection in Concrete Structures (ACI 435R-95),” American Concrete Institute, Farmington Hills, MI, 1995, 89 pp.

14. Gardner, N., “Span/Thickness Limits for Deflection Control,” ACI Structural Journal, V. 108, No. 4, July-Aug. 2011, pp. 453-460.

15. Zhou, F.; Lydon, F.; and Barr, B., “Effect of Coarse Aggregate on Elastic Modulus and Compressive Strength of High Performance Concrete,” Cement and Concrete Research, V. 25, No. 1, 1995, pp. 177-186. doi: 10.1016/0008-8846(94)00125-I

16. Ahmad, S., and Shah, S., “Structural Properties of High Strength Concrete and Its Implications for Precast Prestressed Concrete,” PCI Journal, V. 30, No. 6, 1985, pp. 92-119. doi: 10.15554/pcij.11011985.92.119

17. Barr, P., and Angomas, F., “Differences between Calculated and Measured Long-Term Deflections in a Prestressed Concrete Girder Bridge,” Journal of Performance of Constructed Facilities, ASCE, V. 24, No. 6, 2010, pp. 603-609. doi: 10.1061/(ASCE)CF.1943-5509.0000121

18. Rizkalla, S.; Mirmiran, A.; Zia, P.; Russell, H.; and Mast, R., “Application of the LRFD Bridge Design Specifications to High-Strength Structural Concrete: Flexure and Compression Provisions,” NCHRP Report 595, Transportation Research Board, Washington, DC, 2007, 37 pp.

19. Graybeal, B., and Greene, G., “Lightweight Concrete: Mechanical Properties” Federal Highway Administration No. FHWA-HRT-13-061, McLean, VA, June 2013, 12 pp.

20. Tadros, M.; Al-Omaishi, N.; Seguirant, S.; and Gallt, J., “Prestress Losses in Pretensioned High-Strength Concrete Bridge Girders,” NCHRP Report 496, Transportation Research Board, Washington, DC, 2003, 73 pp.

21. ACI Committee 363, “Report on High-Strength Concrete (ACI 363R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 69 pp.

22. Noguchi, T.; Tomosawa, F.; Nemati, K. M.; Chiaia, B. M.; and Fantilli, A. P., “A Practical Equation for Elastic Modulus of Concrete,” ACI Structural Journal, V. 103, No. 5, Sept.-Oct. 2009, pp. 690-696.

23. Cetin, A., and Carrasquillo, R., “High-Performance Concrete: Influence of Coarse Aggregates on Mechanical Properties,” ACI Materials Journal, V. 95, No. 3, May-June 1998, pp. 252-259.

24. Iravani, S., “Mechanical Properties of High-Performance Concrete,” ACI Materials Journal, V. 93, No. 5, Sept.-Oct. 1996, pp. 416-426.

25. Logan, A.; Choi, W.; Mirmiran, A.; Rizkalla, S.; and Zia, P., “Short-Term Mechanical Properties of High-Strength Concrete,” ACI Materials Journal, V. 106, No. 5, Sept.-Oct. 2009, pp. 413-418.

26. Bilir, T., “Investigation of Performances of Some Empirical and Composite Models for Predicting the Modulus of Elasticity of High Strength Concretes Incorporating Ground Pumice and Silica Fume,” Construction and Building Materials, V. 127, 2016, pp. 850-860. doi: 10.1016/j.conbuildmat.2016.10.054

27. Mostofinejad, D., and Nozhati, M., “Prediction of the Modulus of Elasticity of High Strength Concrete,” Indian Journal of Science and Technology, V. 29, 2005, pp. 311-321.

28. Malhotra, V.; Zhang, M.; Read, P.; and Ryell, J., “Long-Term Mechanical Properties and Durability Characteristics of High-Strength/High-Performance Concrete Incorporating Supplementary Cementing Materials under Outdoor Exposure Conditions,” ACI Materials Journal, V. 97, No. 5, Sept.-Oct. 2000, pp. 518-525.

29. FDOT, Standard Specifications for Road and Bridge Construction Section 346, Florida Department of Transportation, Tallahassee, FL, 2016, pp. 315-335.

30. Pauw, A., “Static Modulus of Elasticity of Concrete as Affected by Density,” Journal Proceedings, V. 57, No. 12, Dec. 1960, pp. 679-688.

31. AASHTO LRFD Bridge Design Specifications, seventh edition, American Association of State Highway and Transportation Officials, Washington, DC, 2014, 245 pp.

32. Ivan Diaz-Loya, E.; Allouche, E.; and Vaidya, S., “Mechanical Properties of Fly-Ash-Based Geopolymer Concrete,” ACI Materials Journal, V. 108, No. 3, May-June 2011, pp. 300-306.

33. Martí-Vargas, J.; Caro, L.; and Serna-Ros, P., “Size Effect on Strand Bond and Concrete Strains at Prestress Transfer,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2013, pp. 419-430.

34. Jurowski, K., and Grzeszczyk, S., “The Influence of Concrete Composition on Young’s Modulus,” Procedia Engineering, V. 108, 2015, pp. 584-591. doi: 10.1016/j.proeng.2015.06.181

35. ACI Committee 214, “Guide to Evaluation of Strength Test Results of Concrete (ACI 214R-11),” American Concrete Institute, Farmington Hills, MI, 2011, 20 pp.

36. Ozyildirim, C., “Comparison of Air Void Content Measurements in Fresh versus Hardened Concretes,” Virginia Department of Transportation No. VTRC 90-R23, Mar. 1990, 32 pp.

37. Weiss, J., “Elastic Properties, Creep, and Relaxation,” Significance of Tests and Properties of Concrete and Concrete-Making Materials, ASTM International, West Conshohocken, PA, 2006, pp. 194-206.

38. ASTM C33/C33M-16, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2016, 11 pp.

39. ASTM C39/C39M-15, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2015, 7 pp.

40. ASTM C469/C469M-144, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014, 5 pp.

41. Malhotra, V., and Carino, N., “The Maturity Method,” Handbook on Nondestructive Testing of Concrete, second edition, CRC Press, Boca Raton, FL, 2004, pp. 5-1 – 5-47.

42. Gajda, J., “Mass Concrete for Buildings and Bridges,” EB547, Portland Cement Association, Skokie, IL, 2007, 44 pp.

43. Bentz, D.; Jones, S.; Stutzman, P.; Arnold, J.; Boisclair, M.; Rothfeld, P.; Tanesi, J.; Kim, H.; Munoz, J.; and Beyene, M., “Influence of Aggregate Characteristics on Concrete Performance,” Technical Note (NIST TN)-1963, May 2017, 109 pp.

44. Aïtcin, P., and Mehta, P., “Effect of Coarse Aggregate Characteristics on Mechanical Properties of High-Strength Concrete,” ACI Materials Journal, V. 87, No. 2, Mar.-Apr. 1990, pp. 103-107.

45. Akçaoğlu, T.; Tokyay, M.; and Çelik, T., “Effect of Coarse Aggregate Size and Matrix Quality on ITZ and Failure Behavior of Concrete under Uniaxial Compression,” Cement and Concrete Composites, V. 26, No. 6, 2004, pp. 633-638. doi: 10.1016/S0958-9465(03)00092-1

46. Kong, L.; Zhang, B.; Ge, Y.; and Yuan, J., “Effect of Ceramsite Structure on Microstructure of Interfacial Zone and Durability of Combined Aggregate Concrete,” Journal of Wuhan University of Technology-Mater, Science Editor, V. 24, No. 1, Feb. 2009, pp. 145-149.

47. Wu, K.; Chen, B.; Yao, W.; and Zhang, D., “Effect of Coarse Aggregate Type on Mechanical Properties Of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 10, 2001, pp. 1421-1425. doi: 10.1016/S0008-8846(01)00588-9

48. Rich, D., “Porosity in Oolitic Limestones,” PhD dissertation, University of Illinois at Urbana-Champaign, Urbana, IL, 1980, 195 pp.

49. Ferraro, C. and Watts, B., “Development of Design Parameters for Virtual Cement and Concrete Testing,” Florida Department of Transportation No. BDK75 977-73, Tallahassee, FL, Dec. 2013, 133 pp.

50. Lo, T., and Cui, H., “Effect of Porous Lightweight Aggregate on Strength of Concrete,” Materials Letters, V. 58, No. 6, 2004, pp. 916-919. doi: 10.1016/j.matlet.2003.07.036

51. Perry, C., and Gillott, J., “The Influence of Mortar-Aggregate Bond Strength on the Behaviour of Concrete in Uniaxial Compression,” Cement and Concrete Research, V. 7, No. 5, 1977, pp. 553-564. doi: 10.1016/0008-8846(77)90117-X


ALSO AVAILABLE IN:

Electronic Structural Journal