Title: Prediction of Drying Shrinkage Cracks of Steel Chip Reinforced Polymer Cement Mortar

Author(s): Yuika Ida, Sunhee Hong, Shinya Kimura, Yuichi Sato, Yoshio Kaneko

Publication: JCI

Volume: 14

Issue: 12

Appears on pages(s): 739 - 752

Keywords:

DOI: 10.3151/jact.14.739

Date: 1/1/2016