Title: Modeling of Chloride Transport Resistance in Cement Hydrates by Focusing on Nanopores

Author(s): Yuya Takahashi, Tetsuya Ishida

Publication: JCI

Volume: 14

Issue: 11

Appears on pages(s): 728 - 738

Keywords:

DOI: 10.3151/jact.14.728

Date: 1/1/2016