Title: Combined Effects of Temperature and Irradiation on Concrete Damage

Author(s): Yann Le Pape, Alain Giorla, Julien Sanahuja

Publication: JCI

Volume: 14

Issue: 3

Appears on pages(s): 70 - 86

Keywords:

DOI: 10.3151/jact.14.70

Date: 1/1/2016

Abstract: