International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Performance of RC Columns with Wide Hoop Spacing at Mechanical Splices

Author(s): Syafri Wardi, Yasushi Sanada, Yuebing Li, Hiroshi Kuramoto, Tomohiro Adachi, Shunichiro Murayama

Publication: JCI

Volume: 14

Issue: 9

Appears on pages(s): 521 - 534

Keywords:

DOI: 10.3151/jact.14.521

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »