Title: Autogenous Shrinkage and Expansion Related to Compressive Strength and Concrete Composition

Author(s): Elica Marušić, Nina Štirmer

Publication: JCI

Volume: 14

Issue: 9

Appears on pages(s): 489 - 501

Keywords:

DOI: 10.3151/jact.14.489

Date: 1/1/2016

Abstract: