Title: Numerical Strategy for Forecasting the Leakage Rate of Inner Containments in Double-Wall Nuclear Reactor Buildings

Author(s): Mehdi Asali, Bruno Capra, Jacky Mazars, Jean-Baptiste Colliat

Publication: JCI

Volume: 14

Issue: 8

Appears on pages(s): 408 - 420

Keywords:

DOI: 10.3151/jact.14.408

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access