Title: Effect of Load Pattern in the Generation of Higher Harmonic Amplitude in Concrete Using Nonlinear Ultrasonic Test

Author(s): Jason Maximino C. Ongpeng, Winston C. Oreta, Sohichi Hirose

Publication: JCI

Volume: 14

Issue: 5

Appears on pages(s): 205 - 214

Keywords:

DOI: 10.3151/jact.14.205

Date: 1/1/2016