Title: Study on Concrete for Civil Engineering Structures Using High Volume Blast Furnace Slag Cement

Author(s): Manabu Hashimoto, Noboru Sakata, Etsuo Sakai, Toshio Yonezawa, Daisuke Hayashi, Toshiyuki Muronoi

Publication: JCI

Volume: 14

Issue: 4

Appears on pages(s): 163 - 171

Keywords:

DOI: 10.3151/jact.14.163

Date: 1/1/2016