Title: Early Hydration of Portland Cement Admixed with Polycarboxylates Studied Under Terrestric and Microgravity Conditions

Author(s): Lei Lei, Markus R. Meier, Alexander Rinkenburger, Baicun Zheng, Lefeng Fu, Johann Plank

Publication: JCI

Volume: 14

Issue: 3

Appears on pages(s): 102 - 107

Keywords:

DOI: 10.3151/jact.14.102

Date: 1/1/2016

Abstract:


Japan Concrete Institute, International Partner Access