Title: Mechanism of Change in Splitting Tensile Strength of Concrete during Heating or Drying up to 90°C

Author(s): Mao Lin, Mitsuki Itoh, Ippei Maruyama

Publication: JCI

Volume: 13

Issue: 2

Appears on pages(s): 94 - 102

Keywords:

DOI: 10.3151/jact.13.94

Date: 1/1/2015