Title: Numerical Approach towards Aging Management of Concrete Structures: Material Strength Evaluation in a Massive Concrete Structure under One-Sided Heating

Author(s): Ippei Maruyama, Go Igarashi

Publication: JCI

Volume: 13

Issue: 11

Appears on pages(s): 500 - 527