Title: Quantitative Evaluation of Crack Resistance Mechanism of Blast Furnace Slag Blended Cement Concrete via Restrained Shrinkage Stress Analysis

Author(s): Tetsushi Kanda, Haruki Momose, Kei-ichi Imamoto, Chizuru Kiyohara, Kohsuke Ishizeki

Publication: JCI

Volume: 13

Issue: 9

Appears on pages(s): 421 - 437

Keywords:

DOI: 10.3151/jact.13.421

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access