Title: Prediction of Drying Shrinkage Cracking of Eco-efficient Steel Chip Reinforced Cementitious Composite Considering Tensile Creep

Author(s): Sunhee Hong, Yuichi Sato, Yoshio Kaneko, Shinya Kimura

Publication: JCI

Volume: 13

Issue: 8

Appears on pages(s): 393 - 402

Keywords:

DOI: 10.3151/jact.13.393

Date: 1/1/2015